Titanium carbide/titanium dioxide/molybdenum sulfide composite material as well as preparation method and application thereof
A technology of titanium dioxide and composite materials, applied in catalyst activation/preparation, chemical instruments and methods, chemical/physical processes, etc., can solve the problems of high price and low output, and achieve the effect of excellent photolysis water hydrogen production rate
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0056] A preparation method of titanium carbide / titanium dioxide / molybdenum sulfide composite material, comprising the steps of:
[0057] (1) Measure 100 milliliters of hydrofluoric acid solution with a mass fraction of 40%, weigh 1 gram of titanium-aluminum-carbon powder, fully mix the hydrofluoric acid solution and titanium-aluminum-carbon powder and stir at room temperature for 72 hours to prepare the first A mixed solution; then filter the first mixed solution, and the precipitate obtained is titanium carbide with MXene material structure, the titanium carbide is a lamellar structure, and its particle size is about 200 mesh;
[0058] (2) 100 milligrams of titanium carbide and 10 milligrams of sodium fluoroborate in step (1) were added to 10 milliliters of hydrochloric acid solution with a concentration of 1 mol / L, and magnetically stirred for 30 minutes to prepare the second mixed solution;
[0059] (3) Put the second mixed solution of step (2) in a hydrothermal reaction k...
Embodiment 2
[0064] A kind of preparation method of titanium carbide / titanium dioxide / molybdenum sulfide composite material, with embodiment 1, difference is: in step (4), get the precipitate of 60 milligrams of steps (3), mix it with 8.1 milligrams of molybdenum trioxide solution and 23.15 mg of potassium thiocyanate was added to deionized water, and magnetically stirred for 60 minutes to prepare a fourth mixed solution.
Embodiment 3
[0066] A kind of preparation method of titanium carbide / titanium dioxide / molybdenum sulfide composite material, with embodiment 1, difference is: in step (4), get the precipitate of 60 milligrams of steps (3), mix it with 13.5 milligrams of molybdenum trioxide solution and 38.6 mg of potassium thiocyanate was added to deionized water, and magnetically stirred for 60 minutes to prepare a fourth mixed solution.
PUM
| Property | Measurement | Unit |
|---|---|---|
| Thickness | aaaaa | aaaaa |
| Width | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com