Intercepting type antirust film and preparation method thereof
An interception and film technology, applied in the field of interception antirust film and its preparation, can solve the problems of poor physical strength and antirust performance, and achieve the effect of all-round improvement in protection performance, heat resistance improvement and health assurance.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0026] Further, the preparation method of the above intercepting anti-rust film comprises the following steps:
[0027] S1. Add the nano-montmorillonite, nano-metal powder, and low-density polyethylene in the first masterbatch to the high-speed mixer, mix for 3-5 minutes, and add industrial white oil and coupling agent during the mixing process;
[0028] S2. Add the gas-phase corrosion inhibitor and low-density polyethylene in the second masterbatch to the high-speed mixer, mix for 3-5 minutes, and add polyethylene wax during the mixing process;
[0029] S3. Take out the first masterbatch and the second masterbatch that have been mixed in step S1 and step S2, and add them to the twin-screw extruder for extrusion and granulation respectively. The set temperature of each section of the twin-screw extruder is : One stage: 173°C, two stage: 171°C, three stage: 167°C, four stage: 172°C, five stage: 179°C, six stage: 185°C, seven stage: 180°C, eight stage: 176°C, nine stage: 175°C,...
Embodiment 1
[0033] Embodiment 1: 50g of the first masterbatch, 50g of the second masterbatch, 900g of auxiliary additives, 37.5g of low-density polyethylene in the first masterbatch, 5g of nano-metal powder, 2.5g of nano-montmorillonite, 5g of gas phase corrosion inhibitor, Add nano-montmorillonite, nano-metal powder, and low-density polyethylene in the first masterbatch to a high-speed mixer, mix for 3-5 minutes, and add industrial white oil and coupling agent during the mixing process; the second masterbatch 40g of low-density polyethylene and 10g of gas-phase corrosion inhibitor in the material, add the gas-phase corrosion inhibitor and low-density polyethylene in the second masterbatch to the high-speed mixer, mix for 3-5 minutes, and add Polyethylene wax; the first and second masterbatches that have been mixed are taken out, respectively added to the twin-screw extruder for extrusion and granulation, and the set temperature of each section of the twin-screw extruder is: first section:...
Embodiment 2
[0034] Example 2, 50g of the first masterbatch, 50g of the second masterbatch, 900g of auxiliary additives, 47g of low-density polyethylene in the first masterbatch, 1.25g of nano-metal powder, 0.5g of nano-montmorillonite, and 1.25g of gas-phase corrosion inhibitor , adding nano-montmorillonite, nano-metal powder, and low-density polyethylene in the first masterbatch to the high-speed mixer, mixing for 3-5 minutes, adding industrial white oil and coupling agent during the mixing process; the second 47.5g of low-density polyethylene and 2.5g of gas-phase corrosion inhibitor in the masterbatch, add the gas-phase corrosion inhibitor and low-density polyethylene in the second masterbatch to the high-speed mixer, mix for 3-5 minutes, and Polyethylene wax is added during the process; the mixed first masterbatch and second masterbatch are taken out, respectively added to the twin-screw extruder for extrusion and granulation, and the set temperature of each section of the twin-screw e...
PUM

Abstract
Description
Claims
Application Information

- R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com