Processing method for enhancing fluffiness of white duck down
A processing method, the technology of white duck down, which is applied in the field of down processing, can solve the problems of affecting the comfort of down products, the breakage of down fibers, and the deterioration of bulkiness, so as to achieve good waterproof effect, maintain bulkiness, and reduce irritation.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0018] A processing method for enhancing the bulkiness of white duck down, comprising the steps of:
[0019] S1. Mix 30kg of ferric chloride hexahydrate, 23kg of ferrous sulfate heptahydrate, and 80kg of water, heat up to 92°C and stir for 20 minutes, add 15kg of ammonia water with a concentration of 20wt% and stir evenly, add 15kg of humic acid, 4kg of whey protein and continue stirring 50min, heat up to 120°C, add 10kg of mercaptoethanol and continue to stir for 5min, the stirring pressure is 24MPa, remove mercaptoethanol, cool, filter, wash until neutral, and dry to obtain the prefabricated material;
[0020] S2. Wash and dry 34kg of white duck down, add 6kg of prefabricated materials, 0.1kg of sodium cocoyl isethionate, 2kg of laurel essential oil, 0.4kg of sodium lauryl sulfate, and 150kg of water, mix evenly, soak for 1 hour, and filter. Washing to obtain pretreated white duck down;
[0021] S3, drying the pretreated white duck down for 200 minutes at a drying temperatu...
Embodiment 2
[0023] A processing method for enhancing the bulkiness of white duck down, comprising the steps of:
[0024] S1. Mix 40kg of ferric chloride hexahydrate, 15kg of ferrous sulfate heptahydrate, and 120kg of water, heat up to 84°C and stir for 40 minutes, add 12kg of ammonia water with a concentration of 23wt% and stir evenly, add 10kg of humic acid, 10kg of whey protein and continue stirring 20min, heat up to 130°C, add 4kg of mercaptoethanol and continue to stir for 12min, the stirring pressure is 12MPa, remove mercaptoethanol, cool, filter, wash until neutral, and dry to obtain the prefabricated material;
[0025] S2. Wash and dry 54kg of white duck down, add 2kg of prefabricated materials, 0.4kg of sodium cocoyl isethionate, 1kg of laurel essential oil, 1kg of sodium lauryl sulfate, and 120kg of water, mix evenly, soak for 2 hours, filter, and wash Obtain pretreated white duck down;
[0026] S3, drying the pretreated white duck down for 160 minutes at a drying temperature of...
Embodiment 3
[0028] A processing method for enhancing the bulkiness of white duck down, comprising the steps of:
[0029] S1. Mix 33kg of ferric chloride hexahydrate, 20kg of ferrous sulfate heptahydrate, and 90kg of water, heat up to 90°C and stir for 25 minutes, add 14kg of ammonia water with a concentration of 21wt% and stir evenly, add 14kg of humic acid, 6kg of whey protein and continue stirring After 40 minutes, heat up to 122°C, add 8kg of mercaptoethanol and continue stirring for 6 minutes, the stirring pressure is 20MPa, remove mercaptoethanol, cool, filter, wash until neutral, and dry to obtain the prefabricated material;
[0030] S2. Wash and dry 40kg of white duck down, add 5kg of prefabricated materials, 0.2kg of sodium cocoyl isethionate, 1.8kg of laurel essential oil, 0.6kg of sodium lauryl sulfate, and 140kg of water, mix evenly, and soak for 1.2h. Filter and wash to obtain pretreated white duck down;
[0031] S3, drying the pretreated white duck down for 180 minutes at a ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com