Graphene composite fiber and cashmere fiber blended yarn production method
A graphene composite, cashmere fiber technology, applied in yarn, textiles and papermaking, etc., can solve the problems of lack of individual selling points and insufficient differentiation
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0014] Embodiment 1: a kind of production method of graphene composite fiber and cashmere fiber blended yarn: comprise the following steps: step A: by mass percentage, select 50% graphene composite fiber and 50% cashmere fiber to mix and form blended fiber , wherein the ratio of the fineness of the graphene composite fiber to the average fineness of the cashmere fiber is 90%~, the ratio of the length of the quantum energy fiber to the average length of the cashmere fiber is 95%; the graphene composite fiber is graphene nylon fiber. The cashmere fiber has a fineness of 21 μm to 24 μm and a fiber length of 30 mm to 38 mm. Step B: Blending the blended fibers. When blending, the cashmere fibers are first mixed, layered and beaten twice, then a blending agent is added, and the wool is beaten again. Then, the cashmere fibers are bagged and stuffed for more than 12 hours, and finally Add the graphene composite fiber layup and mix at least 2 times; in step B, the wool blending agent i...
Embodiment 2
[0017] Embodiment 2: a kind of production method of graphene composite fiber and cashmere fiber blended yarn: comprise the following steps: step A: by mass percentage, select 40% graphene composite fiber and 60% cashmere fiber to mix and form blended fiber , wherein the ratio of the fineness of the graphene composite fiber to the average fineness of the cashmere fiber is 120%, and the ratio of the length of the quantum energy fiber to the average length of the cashmere fiber is 105%; the graphene composite fiber is graphene nylon fiber. The cashmere fiber has a fineness of 21 μm to 24 μm and a fiber length of 30 mm to 38 mm. Step B: Blending the blended fibers. When blending, the cashmere fibers are first mixed, layered and beaten twice, then a blending agent is added, and the wool is beaten again. Then, the cashmere fibers are bagged and stuffed for more than 12 hours, and finally Add graphene composite fiber layer and mix at least 2 times; and hair agent includes and hair oi...
Embodiment 3
[0020]Embodiment 3: a kind of production method of graphene composite fiber and cashmere fiber blended yarn: comprise the following steps: step A: by mass percentage, select 45% graphene composite fiber and 55% cashmere fiber to mix and form blended fiber , wherein the ratio of the fineness of graphene composite fibers to the average fineness of cashmere fibers is 100%, the ratio of the length of quantum energy fibers to the average length of cashmere fibers is 100%; the graphene composite fibers are graphene nylon fibers. The cashmere fiber has a fineness of 21 μm to 24 μm and a fiber length of 30 mm to 38 mm. Step B: Blending the blended fibers. When blending, the cashmere fibers are first mixed, layered and beaten twice, then a blending agent is added, and the wool is beaten again. Then, the cashmere fibers are bagged and stuffed for more than 12 hours, and finally Add graphene composite fiber layer and mix at least 2 times; and hair agent includes and hair oil FX-905 and a...
PUM
Property | Measurement | Unit |
---|---|---|
Fineness | aaaaa | aaaaa |
Fiber length | aaaaa | aaaaa |
Length | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com