Electrochemical device and electric equipment
An electrochemical and isolation layer technology, applied in the field of electrochemical devices and electrical equipment, can solve the problems of low safety performance, large adhesion between the isolation layer and the pole piece, etc., to improve energy density, improve lithium deposition phenomenon, improve The effect of the cyclic expansion phenomenon
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0086] The embodiment of the present application further provides a method for preparing an isolation layer, which is used to prepare at least one of the aforementioned isolation layers. In the following, the material of the isolation layer contains at least polymer fibers as an example, combined with Figure 7 As shown, the preparation method of the isolation layer is described.
[0087] S11: Spraying a solution containing at least a polymer on at least one surface of the positive electrode sheet or the negative electrode sheet by using a spinning process, and drying to form a separation layer.
[0088] S12: Assembling the positive electrode sheet and the negative electrode sheet into an electrochemical device after predetermined treatment.
[0089] The preparation process and materials of the positive electrode sheet and the negative electrode sheet are not limited in the embodiments of the present application.
[0090] In some examples, negative electrode active material ...
Embodiment 1
[0117] (1) Preparation of negative electrode sheet: Mix negative electrode active material graphite, conductive carbon black, and styrene-butadiene rubber in a weight ratio of 96:1.5:2.5, add deionized water, prepare a slurry with a solid content of 0.7, and stir evenly , and then evenly coat the slurry on one surface of the negative electrode collector (such as copper foil), and dry it at 110°C to obtain a negative electrode active material layer, and then use the same process on the other surface of the negative electrode collector Another negative electrode active material layer was formed. Further, after cutting the pieces and welding the tabs, the negative electrode sheet is obtained.
[0118] (2) Preparation of the positive electrode sheet: mix the positive electrode active material lithium cobaltate, conductive carbon black, and polyvinylidene fluoride according to a weight ratio of 97.5:1.0:1.5, add N-methylpyrrolidone as a solvent, and prepare a solid content of 0.75...
Embodiment 2
[0133] The difference from Example 1 is that the polymer fiber on the second surface of the positive electrode sheet is polyimide (PI). The second surface is the surface on which the positive electrode sheet is attached to the solution B, and the first surface is opposite to the second surface.
PUM
| Property | Measurement | Unit |
|---|---|---|
| diameter | aaaaa | aaaaa |
| thickness | aaaaa | aaaaa |
| particle diameter | aaaaa | aaaaa |