[0025] A preparation method of a high-performance water-based special coating for elevator guide rails, the coating comprises the following components in parts by weight, 10 parts of water-based epoxy ester resin, 12 parts of acrylic emulsion, 3 parts of black pigment, 8 parts of anti-rust filler, auxiliary 5 parts of solvent, 0.2 part of drier, 0.8 part of amine neutralizer, 0.9 part of wetting and dispersing agent, 0.1 part of defoamer, 0.3 part of anti-sedimentation aid, 0.2 part of substrate wetting agent, and 1 part of thickener ; Coating preparation method comprises the following steps:
[0026] S1 material preparation: weighing the raw materials of each component;
[0027] S2 Stirring: Add water-based epoxy ester resin to the stirring tank, stir at the first stage speed, add co-solvent, drier, amine neutralizer, and stir at the second stage speed for 20 minutes to make the resin diluted and neutralized evenly; add deionized water, stirring at the third stage speed for ...
Embodiment 2
[0039]A kind of preparation method of high-performance water-based elevator guide rail special coating, its coating comprises the following components by weight, 15 parts of water-based epoxy ester resin, 14 parts of acrylic emulsion, 5 parts of black pigment, 11 parts of antirust filler, auxiliary 8 parts of solvent, 0.4 part of drier, 1.2 parts of amine neutralizer, 1.6 parts of wetting and dispersing agent, 0.3 part of defoamer, 0.5 part of anti-sedimentation aid, 0.4 part of substrate wetting agent, and 1.2 parts of thickener ; Coating preparation method comprises the following steps:
[0040] S1 material preparation: weighing the raw materials of each component;
[0041] S2 Stirring: Add water-based epoxy ester resin to the stirring tank, stir at the first stage speed, add co-solvent, drier, amine neutralizer, and stir at the second stage speed for 20 minutes to make the resin diluted and neutralized evenly; add deionized water, stirring at the third stage speed for 30 m...
Embodiment 3
[0053] A kind of preparation method of high-performance water-based elevator guide rail special coating, its coating comprises the following components by weight, 20 parts of water-based epoxy ester resin, 16 parts of acrylic emulsion, 8 parts of black pigment, 15 parts of antirust filler, auxiliary 10 parts of solvent, 0.6 parts of drier, 1.6 parts of amine neutralizer, 2.4 parts of wetting and dispersing agent, 0.5 parts of defoamer, 0.8 parts of anti-sedimentation aid, 0.5 parts of substrate wetting agent, and 1.5 parts of thickener ; Coating preparation method comprises the following steps:
[0054] S1 material preparation: weighing the raw materials of each component;
[0055] S2 Stirring: Add water-based epoxy ester resin to the stirring tank, stir at the first stage speed, add co-solvent, drier, amine neutralizer, and stir at the second stage speed for 20 minutes to make the resin diluted and neutralized evenly; add deionized water, stirring at the third stage speed fo...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com