Unlock instant, AI-driven research and patent intelligence for your innovation.

Mathod for preparing micro powder containing anti-agglomerated nanometer silver, micro powder produced by the mathod

A nano-silver, micro-powder technology, applied in the fields of botanical equipment and methods, nanotechnology, nanotechnology, etc.

Inactive Publication Date: 2005-10-26
SHENZHEN TSINGHUA YUANXING NANO MATERIAL CO LTD
View PDF6 Cites 1 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

But none of these literature reports involves the use of nano-silver and appropriate carriers as antibacterial materials.

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Image

Smart Image Click on the blue labels to locate them in the text.
Viewing Examples
Smart Image
  • Mathod for preparing micro powder containing anti-agglomerated nanometer silver, micro powder produced by the mathod
  • Mathod for preparing micro powder containing anti-agglomerated nanometer silver, micro powder produced by the mathod
  • Mathod for preparing micro powder containing anti-agglomerated nanometer silver, micro powder produced by the mathod

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0085] Prepare the liquid medicine according to the following amount (based on 10 kg carrier)

[0086] A. Prepare 500 liters of solution A, in which AgNO 3 0.5M, NH 3 h 2 O 0.3M, NaOH 0.1M, the balance is water;

[0087] B. Prepare 50 liters of solution B, in which glucose 4M, HNO 3 0.1M, boil for 1-5 minutes, add ethanol after cooling to make 10M.

[0088] Wash the rush grass, add 98% medical alcohol and distilled water (the ratio of the two is 1:15), soak the rush grass, vacuum extract until the rush grass has no water-soluble organic components and impurities, and dry to obtain solid rush grass particles .

[0089]Mix 10 parts of A+1 part of B (V / V) and let stand for 30 minutes before dipping. Put 10 kg of processed rushes into it. After impregnation, pressurize and homogenize to mix the liquid medicine and the carrier evenly, enter the reaction kettle, add the dispersant 0P-10 continuously under the condition of ventilation and proper stirring, and heat to 150°C un...

Embodiment 2

[0091] Prepare the liquid medicine according to the following amount (based on 10 kg carrier)

[0092] A. Prepare 500 liters of solution A, in which AgNO 3 0.3M, NH 3 h 2 O 0.2M, NaOH 0.07M, the balance is water;

[0093] B. Prepare 50 liters of solution B, in which ascorbic acid 3M, HNO 3 0.1M, boil for 1-5 minutes, add ethanol after cooling to make 10M.

[0094] Wash the rush grass, add 75% medical alcohol and distilled water (the ratio of the two is 1:15), soak the rush grass, vacuum extract until the rush grass has no water-soluble organic components and impurities, and dry to obtain solid rush grass particles .

[0095] Mix 10 parts of A and 1 part of B (V / V) and let it stand for 20 minutes before dipping. Put 10 kg of processed rushes into it. After impregnation, pressurize and homogenize to mix the liquid medicine and the carrier evenly, enter the reaction kettle, add sodium dodecylbenzenesulfonate continuously under ventilation and proper stirring conditions, a...

Embodiment 3

[0097] Prepare the liquid medicine according to the following amount (based on 10 kg carrier)

[0098] A. Prepare 500 liters of solution A, in which AgNO 3 1M, NH 3 h 2 O 0.5M, NaOH 0.3M, the balance is water;

[0099] B. Prepare 50 liters of solution B, in which glucose 8M, HNO 3 0.2M, boil for 1-5 minutes, add ethanol after cooling to make 10M.

[0100] Wash the cotton fibers, add 95% medical alcohol and distilled water (the ratio of the two is 1:15), immerse the cotton fibers, vacuum extract until the cotton fibers are free of water-soluble organic components and impurities, and dry to obtain solid cotton fibers particle.

[0101] After mixing 10 parts of A+1 part of B (V / V), it can be used for impregnation after being placed for 40 minutes, and 10 kg of treated cotton fibers are put into it. After impregnation, pressurize and homogenize to mix the liquid medicine and the carrier evenly, enter the reaction kettle, add tributyl phosphate intermittently under the cond...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

PropertyMeasurementUnit
particle diameteraaaaaaaaaa
sizeaaaaaaaaaa
sizeaaaaaaaaaa
Login to View More

Abstract

The invention relates to a method for preparing micro powder containing anti-agglomerated nanometer silver, a micro powder containing anti-agglomerated nanometer silver and uses of the micro powder. The method of the present invention may prevents strong-active nanometer silver granules from agglomeration. The method included a step of adding dispersant during reaction and step of heat treatment. The micro powder containing anti-agglomerated nanometer silver product by the method of the present invention may serve the function of wide-spectrum antibiosis and diminish inflammation, and may be used as an antiseptic element in pharmacy, medical equipment, medical material, cosmetic, puring water equipment, particularly in commoditis, such as sterilizing in water in spacecraft, aerosol, additives in food and drink, functional components in biological chip, wash, toothpaste, etc.

Description

field of invention [0001] The invention relates to a method for preparing nano-silver, a composite material prepared by the method and an application of the composite material. More specifically, the present invention relates to a method for preparing anti-aggregation nano-silver, the micro-powder containing nano-silver prepared by the method and its use. Background technique [0002] As we all know, nanometer is the unit of length, and 1 nanometer is equal to one billionth of a meter. Nanomaterials usually refer to materials with a particle size between 1 and 100 nanometers, and have special physical and chemical properties that are different from conventional sizes. It is one of the three major technologies of economic development in the 21st century, and it is also the new technology most likely to produce breakthrough achievements. [0003] There are some documents about nano silver and its preparation method in the prior art. For example, the Chinese patent applicatio...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Patents(China)
IPC IPC(8): A01N59/16A61F13/02A61K9/00A61K9/70A61K33/38A61L2/23A61L2/238A61P9/14A61P13/08A61P15/02A61P31/04B22F1/054B22F9/24