Composite antibiotic material in medical use of active carbon fiber-Nano silver, and prepearation method
A technology of activated carbon fiber and antibacterial material is applied in the field of activated carbon fiber-nanosilver composite medical antibacterial material and its preparation, and achieves the effects of good medical application prospect, good performance and simple method.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0031] The preparation steps of activated carbon fiber-nanometer silver composite medical antibacterial material are as follows:
[0032] (1) First put the precursor carbon fiber into the heating furnace to isolate the air and heat and carbonize, so that the hydrogen, oxygen, nitrogen and other components in it are separated and escaped to make carbon fiber, and then the prepared carbon fiber is placed in 35wt% KOH aqueous solution Soak in the medium for 16 hours, take it out, dry and weigh it, put it in the constant temperature zone of the activation furnace, and raise the temperature to the predetermined temperature (700°C) at a heating rate of 5-20°C / min under the protection of nitrogen, and keep the temperature for 20 minutes. , weighed after being taken out under the protection of nitrogen, washed and dried repeatedly, weighed again, calculated fiber yield, and measured specific surface area.
[0033] (2) Take the prepared 2g / L AgNO 3 Put the silver-containing solution i...
Embodiment 2
[0037] The preparation method is the same as in Example 1, except that the carbon fibers are soaked in 10 wt% NaOH aqueous solution for 8 hours, then kept at a constant temperature of 820°C for 50 minutes, cooled under the protection of nitrogen, washed with water, and dried; the activated carbon fibers are immersed in 3g / L silver After 3 hours of ammonium-containing silver ion solution, shake in a 45°C water bath for 20 hours, filter the solution, and rinse the fiber with distilled water.
[0038] (1) First put the precursor carbon fiber into the heating furnace to isolate the air and heat and carbonize, so that the hydrogen, oxygen, nitrogen and other components in it are separated and escaped to make carbon fiber, and then the prepared carbon fiber is placed in 15wt% KOH aqueous solution Soak in the medium for 16 hours, take it out, dry and weigh it, put it in the constant temperature zone of the activation furnace, and raise the temperature to the predetermined temperature ...
Embodiment 3
[0040] To compare the results of traditional wound dressings containing antibiotics, pure carbon fiber materials, mesoporous activated carbon silver-loaded materials, and activated carbon fiber-nano silver composite medical antibacterial materials applied to exudative infected wounds of burned animals.
[0041] The test results are as follows:
[0042] (1) Comparison of antibacterial properties between antibiotics and nano silver
[0043] Items Antibiotics Nanosilver
[0044] Antibacterial spectrum The antibacterial spectrum is different due to different antibiotics, the antibacterial spectrum is broad, and it is not limited by the classification of bacteria
[0045] Usually only against a few types of bacteria
[0046] Has antibacterial effect.
[0047] Drug resistance prone to drug-resistant strains. no resistance
[0048] Drug-resistant bacteria are ineffective, and there is crossover between antibiotics, which have the same bactericidal effect
[0049...
PUM
Property | Measurement | Unit |
---|---|---|
Particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com