A nano-composition and self-microemulsification technology, which is applied in pharmaceutical formulations, emulsion delivery, plant raw materials, etc., can solve the problems of unacceptable by patients, poor affinity of volatile oil, and influence on curative effect, so as to avoid demulsification and increase dispersion , Improve the effect of bioavailability
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0025] Take 2g of mugwort leaf oil and 1g of asarum oil and mix them evenly for later use. Add 3g of polyoxyethylene hydrogenated castor oil and 1g of polysorbate. After mixing evenly, add 200g of water and stir while adding. The inhalation solution of the present invention.
[0026] figure 1 It is a three-phase diagram of oil phase, water phase and surfactant phase. 1 is the microemulsion area, and 2 is the gel area.
[0027] Depend on figure 1 It can be seen that in the gel zone 2, the three-phase mixture is an almost transparent semi-solid that cannot flow freely, and the semi-solid can be put into water and self-emulsify to a viscosity similar to that of water, free-flowing, with little or no Blue fluorescent liquid, in which volatile oil is dispersed in nanometer size (<200nm); in microemulsion zone 1, drug-containing droplets are in nanometer size (within 200nm, more preferably within 100nm), and the viscosity is similar to that of water free-flowing liquid with lit...
Embodiment 2
[0029] Take 2g of mugwort leaf oil and 10g of pepper eye oil, mix well and set aside. Add 15g of polyoxyethylene hydrogenated castor oil and 5g of polysorbate. After mixing evenly, add 200g of water and stir while adding. The inhalation solution of the invention has the effect of rapidly relieving asthma.
Embodiment 3
[0031] Take patchouli oil 5.4g, perilla leaf oil 2.6g, mix well. Add 4 g of polysorbate and 6 g of polyoxyethylene hydrogenated castor oil and homogenize for 10 minutes with a high-speed homogenizer. Add 300g of water, pour in the previously prepared volatile oil mixture, and continue homogenizing for 20 minutes. After being filtered with a 0.45um microporous membrane, it is filled into a brown glass bottle according to the required dose to obtain the oral liquid of the Chinese medicine volatile oil self-microemulsified nano composition of the present invention. The prescription avoids the use of organic solvents in the preparation process, thereby reducing environmental pollution and production costs.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com