Weaving of viscose cotton composite fiber
A composite fiber and composite spinning technology, applied in fiber processing, textiles and papermaking, single-component polyester rayon, etc., can solve the problems of carcinogenicity, great harm to human body, and toxicity of flame-retardant products, and achieve improved temperature buffering and Effects of comfort, good economic and social benefits, increased opportunities for climate regulation
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0011] The preparation method of the present invention is the following steps:
[0012] ① Drying: Dry the raw materials polyester and nylon in a low-temperature dryer for 20-25 minutes;
[0013] ② Melting: Make cellulose into alkali cellulose, chemically react with carbon disulfide to generate cellulose sulfonate, dissolve cellulose sulfonate in dilute sulfuric acid solution to obtain viscose solution, add 5% to 15% Oustlast microcapsules , the solid content accounts for 45% to 55% of the total weight of the solution, the solution temperature is 45±5°C, and the polyamide-6 (nylon 6) spinning solution is prepared by the melt spinning method, and the aminocarboxylic acid in the spinning solution has a lot of weight In 85% spinning melt;
[0014] ③. Spinning: put the viscose spinning solution and the polyamide spinning melt into the spinning box of the DDF-C composite spinning machine at a ratio of 65 / 35 to 35 / 65, and spin through the skin-core composite spinning The board is s...
Embodiment 1
[0018] Ingredients: 60-85 parts of polyester, 15-30 parts of nylon, 5%-6% lye;
[0019] Preparation:
[0020] ① Drying: Dry the raw materials polyester and nylon in a low-temperature dryer for 20-25 minutes;
[0021] ② Melting: Make cellulose into alkali cellulose, chemically react with carbon disulfide to generate cellulose sulfonate, dissolve cellulose sulfonate in dilute sulfuric acid solution to obtain viscose solution, add 5% to 15% Oustlast microcapsules , the solid content accounts for 45% to 55% of the total weight of the solution, the solution temperature is 45±5°C, and the polyamide-6 (nylon 6) spinning solution is prepared by the melt spinning method, and the aminocarboxylic acid in the spinning solution has a lot of weight In 85% spinning melt;
[0022] ③. Spinning: put the viscose spinning solution and the polyamide spinning melt into the spinning box of the DDF-C composite spinning machine at a ratio of 65 / 35 to 35 / 65, and spin through skin-core composite spinn...
Embodiment 2
[0025] Ingredients: 85 parts of polyester, 30 parts of nylon, 6% lye, the preparation method is the same as that of Example 1.
[0026] In summary, the brocade composite fiber woven by this method is made of fine, clean, and environmentally friendly polyester and nylon, and has good smoothness, slipperiness, stiffness, wrinkle resistance, shrink resistance, and easy washing. And other characteristics, it is suitable for clothing and other close-fitting clothing, which is environmentally friendly and healthy.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com