A filter material, positive charge technology, applied in the direction of filtration separation, separation method, chemical instrument and method, etc., can solve the problems of not being suitable for wide application, high manufacturing cost, inability to clean, etc., and achieve great economic and social benefits, Low-cost, easy-to-regenerate effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0020] To prepare a positive charge coating solution:
[0021] (1) Weigh polyvinyl alcohol amino salt, 3g; water, 97g; adjust the conductivity of the water at about 300μs, and the temperature at about 90°C;
[0022] (2) Put water into the container, then slowly add the weighed polyvinyl alcohol amino salt while stirring, and continue stirring for 10 minutes to prepare a positively charged coating solution.
[0023] The preparation method of described positively charged filter material comprises the steps:
[0024] Material selection and crushing: select natural trees that do not contain fat, sugar, strong chromosomes and are easy to crush, and carry out crushing treatment, and control the length of the material to no more than 70cm;
[0025] Expansion treatment: the above-mentioned arbor that has been crushed is puffed at 350°C and a pressure of 2.5mpa for 18 minutes, and then coarse-grained, crushed and screened, the size is controlled at about 0.5-10 mm, and it is used for ...
Embodiment 2
[0030] To prepare a positive charge coating solution:
[0031] (1) Weighing molecular weight greater than 400,000 hydrolyzed chitosan, 5g; water, 95g; the conductivity of the water is less than about 200 μs, and the temperature is about 40°C;
[0032] (2) Put water into the container, then slowly put in the matching hydrolyzed chitosan while stirring, and continue to stir for 10 minutes to obtain a positively charged coating solution.
[0033] The preparation method of described positively charged filter material comprises the steps:
[0034] Material selection and crushing: choose reeds that do not contain fat, sugar, strong chromosomes and are easy to crush, and carry out crushing treatment, and the length of the material should not exceed 70cm;
[0035] Expansion treatment: the above-mentioned arbor that has been crushed is puffed at 350°C and a pressure of 2.5mpa for 18 minutes, and then coarse-grained, crushed and screened, the size is controlled at about 0.5-10 mm, and ...
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com