Spirodiclofen hot aerosol and preparation method thereof
A thermal mist and spirodiclofen technology, applied in the field of spirodiclofen thermal mist and its preparation, can solve the serious drug resistance of E. six-spotted mite, poor effect of E. six-spotted spider mite, and small effective distribution area and other problems, to achieve good contact effect, high application efficiency, and strong contact effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0033] According to the following weight ratio 5% spirodiclofen thermal spray:
[0034] Spirodifen 5kg
[0035] Alkylphenol polyoxyethylene ether OP-4 3kg
[0036] Span-20 4kg
[0037] Secondary alcohol polyoxyethylene ether 1kg
[0038] Calcium Lauryl Sulfate 2kg
[0039] Simethicone 0.5kg
[0040] Ethylene glycol 1kg
[0041] Dibutylhydroxytoluene 0.5kg
[0042] Triethylene glycol 40kg
[0043] Aromatic second-line oil 43kg
[0044] The preparation method of spirodiclofen hot fog agent: according to the above raw material ratio, put 5kg of spirodiclofen original drug into the stirring kettle, inject 40kg of solvent triethylene glycol into the kettle, if the dissolution is slow, properly heat to 40°C, and start the stirring kettle Stir, while stirring, add surfactant alkylphenol polyoxyethylene ether OP-4 3kg, Span-20 4kg, secondary alcohol polyoxyethylene ether 1kg, calcium lauryl sulfate 2kg, silicone defoamer dimethyl silicone oil 0.5kg, antifreeze agent ethylene ...
Embodiment 2
[0046] According to the following weight ratio 10% spirodiclofen thermal spray:
[0047] Spirodifen 10kg
[0048] Alkylphenol polyoxyethylene ether OP-7 4kg
[0049] Span-80 5kg
[0050] Ning milk 33# 4kg
[0051] Sodium benzyl naphthalene sulfonate formaldehyde condensate 2kg
[0052] Simethicone 1kg
[0053]Ethylene glycol 1kg
[0054] Dibutyl hydroxytoluene 1kg
[0055] Triethylene glycol 30kg
[0056] Cyclohexanone 10kg
[0057] Aromatic second-line oil 32kg
[0058] The preparation method of spirodiclofen hot fog agent: according to the above raw material ratio, put 10kg of spirodiclofen original drug into the stirring kettle, inject 30kg of solvent triethylene glycol and 10kg of cyclohexanone into the kettle, if the dissolution is slow, heat it to 45 ℃, turn on the stirring tank to stir, and add surfactant alkylphenol polyoxyethylene ether OP-74kg, Span-805kg, Ningru 33#4kg, benzyl naphthalene sulfonate sodium formaldehyde condensate 2kg, organic silicon disinfe...
Embodiment 3
[0060] According to the following weight ratio 15% spirodiclofen thermal spray:
[0061] Spirodifen 15kg
[0062] Alkylphenol polyoxyethylene ether OP-10 4kg
[0063] Span-80 7kg
[0064] Ning milk 33# 3kg
[0065] Secondary alcohol polyoxyethylene ether 3kg
[0066] Sodium methylnaphthalenesulfonate formaldehyde condensate 3kg
[0067] Simethicone 1kg
[0068] Ethylene glycol 1.5kg
[0069] Dibutyl hydroxytoluene 1kg
[0070] Triethylene glycol 30kg
[0071] Cyclohexanone 15kg
[0072] Residual oil 16.5kg
[0073] The preparation method of spirodiclofen hot fog agent: according to the above raw material ratio, put 15kg of spirodiclofen original drug into the stirring kettle, inject 30kg of solvent triethylene glycol into the kettle, if the dissolution is slow, properly heat to 50°C, and start the stirring kettle Stir, add surfactant alkylphenol polyoxyethylene ether OP-10 4kg, Span-80 7kg, Ningru 33# 3kg, sodium methylnaphthalene sulfonate formaldehyde condensate 3k...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com