Method for preparing refined quartz sand by washing
A technology of quartz sand and quartz stone, which is applied in the field of washing and producing refined quartz sand, which can solve the problems of many impurities, time-consuming and material-consuming, etc., and achieve the effects of high whiteness, wide application range and saving artificial raw materials
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0025] Embodiment 1, a kind of method for washing and producing refined quartz sand, comprising
[0026] S1. Processing: process the quartz stone ore into coarsely crushed stone with a length of 5cm through a stone crushing machine;
[0027] S2. Sand granulation: crush coarsely crushed stones into sand grains, add water continuously during rolling, the ratio of water to sand grains (weight percentage) = 2:1;
[0028] S3. Sedimentation: water flows into the sedimentation tank with sand, and the sedimentation time is 7 hours; when the sand is completely settled, the water on the surface of the sand is drained away;
[0029] S4. Baking: Transport the grit into the baking room for baking. The baking time is 2 hours to form dry sand, take it out, and cool to room temperature;
[0030] S5. Sieving: Screening with a vibrating sieve to obtain finished fine sand.
[0031] Further, the processing in step S1 further includes:
[0032] S11. The processed stone in step S1 is evenly sent...
Embodiment 2
[0038] Example 2, a method for washing and producing refined quartz sand, the steps of which are mostly the same as in Example 1, the difference is that: step S1 is: the quartz ore is processed into a coarsely crushed quartz sand with a length of 25 cm through a stone crushing machine. stone;
[0039] Step S3. Sedimentation: the water carries the sand into the sedimentation tank, and the sedimentation time is 4 hours; when the sand is completely settled, the water on the surface of the sand is drained away;
[0040] S4. Baking: Transport the grit to the baking room for baking. The baking time is 3 hours to form dry sand. Take it out and cool it to room temperature.
Embodiment 3
[0041] Example 3, a method for washing and producing refined quartz sand, the steps of which are mostly the same as those in Example 1, the difference is that: step S1 is: process the quartz stone ore into coarsely crushed quartz sand with a length of 50 cm through a stone knocking machine stone;
[0042] Step S3. Sedimentation: the water carries the sand into the sedimentation tank, and the sedimentation time is 8 hours; when the sand is completely settled, the water on the surface of the sand is drained away;
[0043] S4. Baking: Transport the grit to the baking room for baking. The baking time is 2.5 hours to form dry sand. Take it out and cool it to room temperature.
[0044] In general, the process of producing quartz sand by water method is roughly as follows: the quartz ore is processed into smaller stones by a stone crushing machine, and then the stones are rolled into sand by stone rollers, and water is continuously added during rolling. Bring the sand into the sedim...
PUM
Property | Measurement | Unit |
---|---|---|
length | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com