Radix dipsaci seed pelletization coating and preparation method thereof
A pelletized coating and seed technology, applied in fertilizer mixture, fertilization device, application, etc., can solve the problems of slow progress in the research of seed coating agents, and achieve good drought resistance and good growth
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Example Embodiment
[0028] Example 1 Study on the selection of pelletized coating materials
[0029] Adhesives: sodium carboxymethyl cellulose (CMC), polyvinyl alcohol (PVA), polyvinylpyrrolidone (PVP), chitosan, 107 glue, polyacrylamide.
[0030] Film forming agents: hydroxypropyl methyl cellulose (HPMC), hydroxypropyl methyl cellulose (HPMC) + polyethylene glycol (PEG), sodium carboxymethyl cellulose, chitosan.
[0031] Pelletizing additives: talc powder, bentonite, bentonite raw ore soil (0.2% peach gum).
[0032] Water retaining agent is (SDL-B-400)
[0033] Test instrument: 5BW50-seed coating / pelletizing machine.
[0034] Prepare different concentrations of adhesive and film-forming agent, see Table 1 and Table 2. Under the condition of (25±1)℃, the pH value is measured with PHS-3S type acidity meter, and the viscosity value is measured with DNJ-1 type rotary viscometer. The sensory observation method is used to investigate the odor, precipitation and layering of the seed coating agent. Take 5 mL of...
Example Embodiment
[0053] Example 2 Selection of different growth regulators 1
[0054] Weigh 500g of Dipsacus seeds, put Dipsacus seeds in a container, stir constantly, and spray the adhesive sodium carboxymethyl cellulose solution with a concentration of 1.5% by weight at the same time as the coating fixed layer is 150mL , The dosage of 1.5% sodium carboxymethyl cellulose solution of adhesive for coating additional layer is 3000-4500mL; use 5BW50-seed coating / pelletizing machine for coating.
[0055] While spraying the adhesive sodium carboxymethyl cellulose solution, slowly add the water-retaining agent SDL-B-400, the pelletized additive weight ratio of 1:1 mixed powder, and the mixed powder also has a 1.5% weight ratio disintegrant carboxylate Sodium methyl starch, the added weight of the mixed powder is 50% of the weight of Dipsacus seeds;
[0056] Take out the seeds, dry them, and put them in a container to complete the fixed layer coating;
[0057] Continue to spray 1.5% adhesive carboxymethyl c...
Example Embodiment
[0067] Example 3 Selection of different growth regulators 2
[0068] Weigh various ingredients according to the weight, and coat them according to the optimal coating method described in Example 2, and cultivate the coated seeds under moisture-preserving conditions. Other conditions are the same as above, and the 30-day germination of each group is counted Rate, experimental method design orthogonal experiment as shown in Table 4 and 5.
[0069] Factor Level Table 4
[0070]
[0071] Table 5 Orthogonal test table (L 18 (3 7 )) and the result
[0072]
[0073] Intuitive analysis shows that the primary and secondary effects of each factor are A> C> D> F> G> E> B; That is, in the growth additives, potassium has the greatest influence on the growth and germination of Dipsacus seeds, followed by ammonium molybdate, and sodium naphthenate the least. Finally, the ratio of the matrix is determined to be A 3 C 2 D 2 F 1 G 2 E 1 B 3 . It is finally determined that the weight ratio of potass...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap