A kind of anti-insect paint for plastic lampshade and preparation method thereof
A lampshade and insect-proof technology, which is applied in the field of coatings, can solve the problem that the lampshade paint does not have insect-proof effect, etc., and achieves the effect of good moisture resistance and beautiful appearance.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0011] This embodiment provides an insect-proof coating for plastic lampshades, which contains the following components in parts by mass: 40 parts of polymer emulsion, 3.4 parts of polysilane, 1 part of xylene, 0.48 parts of polyoxyethylene lauryl ether, 8 parts of pigment, light weight 10 parts of calcium carbonate, 0.4 parts of emulsified silicone oil, 0.3 parts of polyacrylamide, 0.5 parts of 2,4-dihydroxybenzophenone, 0.2 parts of dioctyl phthalate, 0.8 parts of deltamethrin, 8 parts of water; The polymer emulsion contains the following components in parts by mass: 6 parts of ethyl acrylate, 1.2 parts of methacrylic acid, 18 parts of styrene, 0.5 parts of glycidyl methacrylate, 2 parts of sodium alkylbenzenesulfonate, sodium persulfate 0.05 parts, 8 parts of water.
[0012] A kind of preparation step of insect-proof coating for plastic lampshade is as follows:
[0013] (1) Preparation of polymer emulsion: first add sodium alkylbenzenesulfonate, water and sodium persulfate...
Embodiment 2
[0016] This embodiment provides an insect-proof coating for plastic lampshades, which contains the following components in parts by mass: 55 parts of polymerized emulsion, 4.7 parts of polysilane, 1.8 parts of xylene, 0.7 parts of polyoxyethylene lauryl ether, 14 parts of pigment, light 17 parts of calcium carbonate, 1.1 parts of emulsified silicone oil, 0.6 parts of polyacrylamide, 1 part of 2,4-dihydroxybenzophenone, 0.5 parts of dioctyl phthalate, 1.6 parts of deltamethrin, 17 parts of water; The polymer emulsion contains the following components in parts by mass: 6 parts of ethyl acrylate, 1.2 parts of methacrylic acid, 18 parts of styrene, 0.5 parts of glycidyl methacrylate, 2 parts of sodium alkylbenzenesulfonate, sodium persulfate 0.05 parts, 8 parts of water.
[0017] A kind of preparation step of insect-proof coating for plastic lampshade is as follows:
[0018] (1) Preparation of polymer emulsion: first add sodium alkylbenzenesulfonate, water and sodium persulfate i...
Embodiment 3
[0021] This embodiment provides an insect-proof coating for plastic lampshades, which contains the following components in parts by mass: 48 parts of polymerized emulsion, 4 parts of polysilane, 1.4 parts of xylene, 0.62 parts of polyoxyethylene lauryl ether, 11 parts of pigment, light weight 13.5 parts of calcium carbonate, 0.7 parts of emulsified silicone oil, 0.45 parts of polyacrylamide, 0.7 parts of 2,4-dihydroxybenzophenone, 0.35 parts of dioctyl phthalate, 1.2 parts of permethrin, and 13 parts of water; The polymer emulsion contains the following components in parts by mass: 6 parts of ethyl acrylate, 1.2 parts of methacrylic acid, 18 parts of styrene, 0.5 parts of glycidyl methacrylate, 2 parts of sodium alkylbenzenesulfonate, sodium persulfate 0.05 parts, 8 parts of water.
[0022] A kind of preparation step of insect-proof coating for plastic lampshade is as follows:
[0023] (1) Preparation of polymer emulsion: first add sodium alkylbenzene sulfonate, water and sod...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com