[0047] The cement with inorganic additives has the following weight ratio: 70-75 parts by weight of portland cement clinker, 5-10 parts by weight of inorganic additives, and 15-20 parts by weight of gypsum powder. Preferably, the weight ratio is: 72 parts by weight of Portland cement clinker, 8 parts by weight of inorganic additives, and 16 parts by weight of gypsum powder. Described inorganic additive is made by following method:
[0048] a Adjust the moisture content of the sludge to 60-70%,
[0049] b. Low-temperature pyrolysis of the sludge obtained in a. The temperature of the pyrolysis is 200-450°C, and the pyrolysis gas is collected.
[0050] c. Heat the pyrolysis residue after the treatment in step b to 1300~1500°C to burn the organic matter in the sludge to obtain the inorganic additive.
PUM
Property | Measurement | Unit |
---|---|---|
heating value | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com