Problems solved by technology
Method used
Examples
Embodiment 1
[0027] Preparation of pre-prepared resin liquid: In a certain volume of agitable open tank, first add 94.7 parts of 60°C water, then add 5 parts of cellulose resin while stirring, and disperse for 15 minutes with a disc stirring blade at 1000rpm / min; then cool down to Below 30°C, add 0.3 parts of preservative while stirring, and disperse for 10 minutes to obtain a pre-prepared resin solution for later use.
[0028] Mixing, dispersion and tempering: Put 25 parts of pre-prepared resin liquid into the open cylinder, and then put in 20 parts of water-based polyurethane resin, 14.5 parts of inorganic filler, 30 parts of water-based color paste, 5 parts of water-based anti-scratch agent, 0.1 part Water-based defoamer, 5 parts of water-based wetting and leveling agent, dispersed for 8-15 minutes with a disc-type stirring paddle at 1500rpm / min, then adjusted the pH value between 8-9 with 0.4% diethanolamine, and finally checked the viscosity of the output, If the color and appearance ...
Embodiment 2
[0036] Preparation of pre-prepared resin liquid: In a certain volume of agitable open tank, first add 59.9 parts of 60°C water, 5 parts of ethanol, and 5 parts of propylene glycol, and disperse for 5 minutes with a disc-type stirring paddle at 500 rpm / min; add cellulose while stirring 30 parts of resin were dispersed at 800rpm / min for 15 minutes; then the temperature was lowered to below 30°C, 0.1 part of preservative was added while stirring, and dispersed for 10 minutes to obtain a pre-prepared resin solution for later use.
[0037] Mixing, dispersing and tempering: put 70 parts of pre-prepared resin liquid into the open cylinder, and then put in 5 parts of water-based polyurethane resin, 13.6 parts of inorganic filler, 10 parts of water-based color paste, 0.1 part of water-based anti-scratch agent, 0.2 parts Water-based defoamer, 1 part of water-based wetting and leveling agent, disperse for 15 minutes with a disc stirring paddle at 800rpm / min, then use 0.1% diethanolamine t...
Embodiment 3
[0045] Preparation of pre-prepared resin liquid: In a certain volume of agitable open tank, first add 84.95 parts of 60°C water, 2 parts of ethanol, and 3 parts of glycerin, and disperse for 3 minutes with a disc-type stirring paddle at 500 rpm / min; put in while stirring 10 parts of cellulose resin, dispersed at 800rpm / min for 15 minutes; then lower the temperature to below 30°C, add 0.05 parts of preservative while stirring, and disperse for 10 minutes to obtain a pre-prepared resin solution for later use.
[0046] Mixing, dispersing and tempering: put 60 parts of pre-prepared resin liquid into the open cylinder, and then put in 10 parts of water-based polyurethane resin, 12 parts of inorganic filler, 10 parts of water-based color paste, 3 parts of water-based anti-scratch agent, 1 part of Water-based defoaming agent, 3 parts of water-based wetting and leveling agent, disperse for 8-15 minutes with a disc stirring paddle at 800rpm / min, then use 1% diethanolamine to adjust the ...