A kind of preparation method of fuel oil
A fuel oil and raw material technology, applied in the field of chemical raw material preparation, can solve the problems of difficult preparation, unsatisfactory rapid production, and pollution, and achieve the effects of simple and convenient preparation process, obvious use effect and strong adhesion
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0018] A kind of fuel oil, comprises the raw material composition of following weight part:
[0019] Kerosene 6-14kg; vegetable oil 20-40kg, vegetable oleic acid 3-7kg, refined tar 10-16kg, methanol 10-25kg, sodium dodecylbenzene sulfonate 1-8kg, polyisobutylamine 5-15kg, coal oil 85-95kg pulp, 6-10kg lower ether, 0.1-1.0kg scorch inhibitor, 0.5-1.5kg sorbitan fatty acid ester.
[0020] Its preparation method is:
[0021] a. Select a reaction kettle with a stirrer, then add all the kerosene and vegetable oil in the formula to the reaction kettle and start stirring until completely mixed;
[0022] b. Add all the vegetable oleic acid, refined tar and methanol in the raw material into the reaction kettle, stir and heat to 60-80°C, and then react at constant temperature for 2-4h;
[0023] c. After the reaction in the above step b is completed, the temperature of the reaction kettle is lowered to 20-25°C, and the coal-based oil slurry and lower ether in the raw materials are adde...
Embodiment 2
[0027] A kind of fuel oil, comprises the raw material composition of following weight part:
[0028] Kerosene 10kg; vegetable oil 30kg, vegetable oleic acid 5kg, refined tar 14kg, methanol 20kg, stearic acid 4kg, polyisobutylamine 10kg, coal oil slurry 90kg, lower ether 8kg, scorch inhibitor 0.5kg, sorbitan fatty acid Ester 1kg.
[0029] Its preparation method is:
[0030] a. Select a reaction kettle with a stirrer, then add all the kerosene and vegetable oil in the formula to the reaction kettle and start stirring until completely mixed;
[0031] b. Add all the vegetable oleic acid, refined tar and methanol in the raw material into the reaction kettle, stir and heat to 60-80°C, and then react at constant temperature for 2-4h;
[0032] c. After the reaction in the above step b is completed, the temperature of the reaction kettle is lowered to 20-25°C, and the coal-based oil slurry and lower ether in the raw materials are added into it, stirred evenly, and left to stand for 5...
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More