A reactive printing and paste technology, which is applied in dyeing, textiles and papermaking, etc., can solve the problems of composite printing paste printing effect and the inability to improve the depaste rate at the same time, achieve low cost, good stability, and simple preparation method Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0051] The easy-to-wash reactive printing paste of this example was prepared with the raw material components described in Table 1. Among them, the degree of substitution of sodium carboxymethyl cellulose is 1.0, and the degree of substitution of sodium carboxymethyl starch is 1.0.
[0052] The preparation method of the easy-to-wash reactive printing paste includes the following steps:
[0053] At room temperature, add sodium carboxymethyl cellulose, sodium carboxymethyl starch, lithium magnesium silicate, polyvinylpyrrolidone, sodium lauryl sulfate into the cone mixer, start the stirrer, and add the wetting component ( Isomerized tridecyl alcohol polyoxyethylene ether and fatty alcohol polyoxyethylene ether sodium sulfate), the amount of wetting component per minute is 15% (the percentage is the weight percentage of the amount per minute to the total amount of wetting components ), add sodium citrate, sodium gluconate, sodium chloride, and sodium sulfate after stirring for 15 min...
Embodiment 2
[0055] The easy-to-wash reactive printing paste of this example was prepared with the raw material components described in Table 1. Among them, the degree of substitution of sodium carboxymethyl cellulose is 1.2, and the degree of substitution of sodium carboxymethyl starch is 1.0.
[0056] At room temperature, add sodium carboxymethyl cellulose, sodium carboxymethyl starch, lithium magnesium silicate, polyvinylpyrrolidone, sodium lauryl sulfate into the cone mixer, start the stirrer, and add the wetting component ( Isomerized tridecyl alcohol polyoxyethylene ether and fatty alcohol polyoxyethylene ether sodium sulfate), the amount of wetting component per minute is 20% (percentage is the weight percentage of the amount per minute to the total amount of wetting components ), add sodium citrate, sodium gluconate, sodium chloride, and sodium sulfate after stirring for 20 minutes, and stir for 45 minutes.
Embodiment 3
[0058] The easy-to-wash reactive printing paste of this example was prepared with the raw material components described in Table 1. Among them, the degree of substitution of sodium carboxymethyl cellulose is 1.5, and the degree of substitution of sodium carboxymethyl starch is 1.2.
[0059] At room temperature, add sodium carboxymethyl cellulose, sodium carboxymethyl starch, lithium magnesium silicate, polyvinylpyrrolidone, sodium lauryl sulfate into the cone mixer, start the stirrer, and add the wetting component ( Isomerized tridecyl alcohol polyoxyethylene ether and fatty alcohol polyoxyethylene ether sodium sulfate), the amount of wetting component per minute is 20% (percentage is the weight percentage of the amount per minute to the total amount of wetting components ), add sodium citrate, sodium gluconate, sodium chloride, and sodium sulfate after stirring for 10 minutes, and stir for 45 minutes.
PUM
Property | Measurement | Unit |
---|---|---|
degree of substitution | aaaaa | aaaaa |
degree of substitution | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com