An iron safflower glaze and nickel-iron tailings technology, applied in the field of ceramics, can solve the problems of unutilized tailings slag, water and soil loss, waste of resources, etc., and achieve the effects of saving the development of mineral resources, reducing the consumption, and reducing the discharge of solid waste.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
specific Embodiment 1
[0026] A kind of iron safflower glazed porcelain prepared from ferronickel tailings slag,
[0027] The green body formula is prepared by mixing the following parts by weight: 45 parts by weight of ferronickel tailings, 25 clay, 6 pyrophyllite, 6 quartz, 11 potassium albite feldspar, and 7 limestone; the chemical components of the green body formula are as follows: SiO2 56, AL2O3 13, MgO 8, CaO 4, K2O 5, Na2O 4, Fe2O3 6, MnO2 1, TiO2 1, loss on ignition 2.
[0028] The glaze formula is prepared by mixing the following parts by weight: nickel-iron tailings 31, potassium feldspar 25, clay 23, quartz 9, iron oxide 7, phosphorus pentoxide 5; the chemical components of the glaze formula are as follows: SiO2 48, AL2O3 17, MgO 7, CaO 8, K2O6, Na2O 1, Fe2O3 12, P2O5 1.
specific Embodiment 2
[0030] A kind of iron safflower glazed porcelain prepared from ferronickel tailings slag,
[0031] The green body formula is prepared by mixing the following parts by weight: nickel-iron tailings 48, clay 21, pyrophyllite 8, quartz 9, potassium albite feldspar 11, limestone 6; the chemical composition content of the green body formula is as follows: SiO 2 53. AL 2 o 3 13. MgO7, CaO5, K 2 O6, Na2 O 3 , Fe 2 o 3 9. MnO 2 2. Loss on ignition 2.
[0032] The glaze formula is prepared by mixing the following parts by weight: nickel-iron tailings 28, potassium feldspar 29, clay 20, quartz 7, iron oxide 10, phosphorus pentoxide 6; the chemical components of the glaze formula are as follows: SiO 2 43. AL 2 o 3 17. MgO 9, CaO 8, K 2 O8, Na 2 O2, Fe 2 o 3 12. P 2 o 5 1.
specific Embodiment 3
[0034] A kind of iron safflower glazed porcelain prepared from ferronickel tailings slag,
[0035] The green body formula is prepared by mixing the following parts by weight: nickel-iron tailings 42, clay 20, pyrophyllite 6, quartz 10, potassium albite feldspar 14, limestone 8; the chemical composition content of the green body formula is as follows: SiO 2 57. AL 2 o 3 13. MgO 9, CaO 4, K 2 O4, Na 2 O 4, Fe 2 o 3 6. MnO 2 1. Loss on ignition 2.
[0036] The glaze formula is prepared by mixing the following parts by weight: nickel-iron tailings 25, potassium feldspar 28, clay 24, quartz 7, iron oxide 9, phosphorus pentoxide 7; the chemical components of the glaze formula are as follows: SiO 2 49. AL 2 o 3 15. MgO 6, CaO 8, K 2 O8, Na 2 O 1, Fe 2 o 3 12. P 2 o 5 1.
[0037] The iron safflower glaze porcelain prepared by using ferronickel tailings slag and its preparation process provided by the present invention use the ferronickel tailings slag discarde...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com