A rapeseed clubroot and high temperature resistance technology, applied in seed coating/seed dressing, botanical equipment and methods, biocides, etc., can solve the problem of large amount of pesticides, increased human and animal health and safety risks, and clubroot crop rotation To achieve the effects of enhancing stress resistance and storage resistance, prolonging residence and action time, and being easy to use on a large scale
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0056] 1) Prepare 1 part of Pulutong and 80 parts of coating material in parts by weight;
[0057] Described coating material is counted as by weight:
[0058] Acrylic resin 5 parts
[0059] Disodium hydrogen phosphate 20 parts
[0060] 40 parts of kaolin;
[0061] 2) Under stirring conditions, slowly add water to the coating material, the amount of water added is 1.5 times the weight of the coating material, and stir evenly;
[0062] 3) Add the active ingredients and stir evenly;
[0063] 4) Dry at 30-50°C and sieve until the particle size is not greater than 5 microns.
Embodiment 2
[0065] 1) Prepare 5 parts by weight of 6% oligosaccharide·catenin, and 100 parts of coating material;
[0066] Described coating material is:
[0067] Mixture of acrylic resin and povidone 8 parts
[0068] Mixture of disodium hydrogen phosphate and ammonium sulfate 40 parts
[0069] 60 parts of mixture of kaolin and talc;
[0070] Wherein, the mass ratio of acrylic resin and povidone is 3:1; the mass ratio of disodium hydrogen phosphate and ammonium sulfate is 1.5:1; the mass ratio of kaolin and talcum powder is 1:1;
[0071] 2) Under stirring conditions, slowly add water to the coating material, the amount of water added is 1.8 times the weight of the coating material, and stir evenly;
[0072] 3) Add the active ingredients and stir evenly;
[0073] 4) Dry at 30-50°C and sieve until the particle size is not greater than 5 microns.
Embodiment 3
[0075] 1) In parts by weight, prepare 3 parts of 3% Alternaria ultrafines activated protein and 90 parts of coating material;
[0076] Described coating material is:
[0077] Mixture of acrylic resin and povidone 6 parts
[0078] Mixture of disodium hydrogen phosphate and ammonium sulfate 30 parts
[0079] 50 parts of mixture of kaolin and talc;
[0080] Wherein, the mass ratio of acrylic resin and povidone is 4:1; the mass ratio of disodium hydrogen phosphate and ammonium sulfate is 1.8:1; the mass ratio of kaolin and talc is 1.2:1;
[0081] 2) Under stirring conditions, slowly add water to the coating material, the amount of water added is 1.5 times the weight of the coating material, and stir evenly;
[0082] 3) Add the active ingredients and stir evenly;
[0083] 4) Dry at 30-50°C and sieve until the particle size is not greater than 5 microns.
PUM

Abstract
Description
Claims
Application Information

- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com