Examples
Embodiment 1
[0019] A preparation method of damping paint, comprising the following steps:
[0020] 1) Weigh 28 parts of acrylic emulsion, 25 parts of deionized water, put them in a stirring container, add 20 parts of filler, 35 parts of mica powder, 1 part of dispersant, 0.2 parts of defoamer, and 0.2 parts of halogen-free flame retardant , at a rotating speed of 500r / min, after stirring for 20min, a mixed solution was obtained;
[0021] 2) Add 2 parts of film-forming aid, 0.5 part of dispersant, 0.1 part of defoamer, and 0.1 part of halogen-free flame retardant to the mixed liquid obtained in step 1), stir for 10 minutes at a speed of 100 r / min, and then add The thickener can be used after adjusting the consistency.
Embodiment 2
[0023] A preparation method of damping paint, comprising the following steps:
[0024] 1) Weigh 35 parts of acrylic emulsion and 32 parts of deionized water, put them in a stirring container, add 40 parts of filler, 45 parts of mica powder, 3 parts of dispersant, 0.8 parts of defoamer, and 0.8 parts of halogen-free flame retardant , at a rotating speed of 800r / min, after stirring for 28min, a mixed solution was obtained;
[0025] 2) Add 2 parts of film-forming aids, 1 part of dispersant, 0.3 parts of defoamer, and 0.3 parts of halogen-free flame retardant to the mixed liquid obtained in step 1). Stir for 15 minutes at a speed of 110 r / min before adding The thickener can be used after adjusting the consistency.
Embodiment 3
[0027] A preparation method of damping paint, comprising the following steps:
[0028] 1) Weigh 30 parts of acrylic emulsion, 30 parts of deionized water, put them in a stirring container, add 25 parts of filler, 40 parts of mica powder, 1.5 parts of dispersant, 0.5 parts of defoamer, and 0.6 parts of halogen-free flame retardant , at a rotating speed of 600r / min, after stirring for 22min, a mixed solution was obtained;
[0029] 2) Add 7 parts of film-forming aids, 1.2 parts of dispersants, 0.2 parts of defoamers, and 0.4 parts of halogen-free flame retardants to the mixture obtained in step 1). Stir for 16 minutes at a speed of 110 r / min before adding The thickener can be used after adjusting the consistency.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com