Method for manufacturing nickel-ion-chromium alloy seamless tube

A technology of nickel-iron-chromium alloy and manufacturing method, which can be applied to coatings, anti-corrosion coatings, polycarbonate coatings, etc., can solve the problem that seamless metal pipes need to be improved, and achieve the effect of excellent corrosion resistance

Inactive Publication Date: 2016-01-27
SUZHOU BEST METAL PROD
View PDF2 Cites 0 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0002] The corrosion resistance, rust resistance and weather r

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0014] A method for manufacturing a nickel-iron-chromium alloy seamless pipe, comprising the step of attaching a metal protective coating to the metal pipe main body, and the metal protective coating is composed of the following components in parts by weight:

[0015] 1-2 parts of pentaerythritol, 8.7 parts of modified polybutadiene resin, 2.3 parts of ethylene bis stearamide, 0.9 parts of dibromomethane, 0.9 parts of castor oil, 0.8 parts of titanium dioxide, 0.4 parts of silicon dioxide, 1.8 parts of poly Carbonate.

Embodiment 2

[0017] A method for manufacturing a nickel-iron-chromium alloy seamless pipe, comprising the step of attaching a metal protective coating to the metal pipe main body, and the metal protective coating is composed of the following components in parts by weight:

[0018] 1 part of pentaerythritol, 8.7 parts of modified polybutadiene resin, 2.3 parts of ethylene bisstearamide, 0.9 parts of methylene bromide, 0.9 parts of castor oil, 0.8 parts of titanium dioxide, 0.4 parts of silica, 1.8 parts of polycarbonate .

Embodiment 3

[0020] A method for manufacturing a nickel-iron-chromium alloy seamless pipe, comprising the step of attaching a metal protective coating to the metal pipe main body, and the metal protective coating is composed of the following components in parts by weight:

[0021] 2 parts of pentaerythritol, 8.7 parts of modified polybutadiene resin, 2.3 parts of ethylene bis stearamide, 0.9 parts of methylene bromide, 0.9 parts of castor oil, 0.8 parts of titanium dioxide, 0.4 parts of silica, 1.8 parts of polycarbonate .

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

No PUM Login to view more

Abstract

The invention discloses a method for manufacturing a nickel-ion-chromium alloy seamless tube. The method comprises the step of attaching a metal tube main body to a metal protective coating. The metal protective coating comprises the following components in parts by weight: 1-2 parts of pentaerythritol, 8.7 parts of a modified polybutadiene resin, 2.3 parts of ethylene distearamide, 0.9 part of dibromomethane, 0.8 part of titanium dioxide, 0.4 part of silicon dioxide and 1.8 parts of polycarbonate. According to the method for manufacturing the nickel-ion-chromium alloy seamless tube disclosed by the invention, the metal protective coating is attached to the metal tube main body, and the metal tube main body has excellent corrosion resistance, rust resistance and weather resistance.

Description

technical field [0001] The invention relates to a method for manufacturing a nickel-iron-chromium alloy seamless pipe. Background technique [0002] The corrosion resistance, rust resistance and weather resistance of the existing seamless metal pipes all need to be improved. Contents of the invention [0003] The object of the present invention is to provide a manufacturing method of nickel-iron-chromium alloy seamless pipe, in which a metal protective coating is attached to the main body of the metal pipe, and the main body of the metal pipe has excellent corrosion resistance, rust resistance and weather resistance. [0004] In order to achieve the above object, the technical solution of the present invention is to design a method for manufacturing a nickel-iron-chromium alloy seamless pipe, which includes the step of attaching a metal protective coating to the metal pipe main body. In parts by weight, the metal protective coating consists of Composed of the following co...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
IPC IPC(8): C09D147/00C09D169/00C09D191/00C09D7/12C09D5/08
Inventor 王清明
Owner SUZHOU BEST METAL PROD
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products