A kind of ultra-high molecular weight polyethylene anticorrosion tray
An ultra-high molecular weight, polyethylene technology, applied in the field of polymer materials, can solve problems such as processing difficulties, and achieve the effects of solving processing difficulties, improving mechanical strength properties and corrosion resistance, and improving compatibility.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0022] This embodiment is an ultra-high molecular weight polyethylene anticorrosive tray, which is mainly made of the following parts by weight of raw materials:
[0023] Ultra-high molecular weight polyethylene: 93; polylactic acid: 4.0; polyisobutylene: 0.2; silicone rubber: 0.1; kaolin: 0.3; silica: 0.2; rheological processing aid potassium fluoride: 0.1; inorganic filler graphite: 10 ; And the molecular weight of UHMWPE is 3.2 million.
[0024] The tray can be made according to conventional methods in the art. More specifically, the manufacturing method of the tray in this embodiment is as follows:
[0025] Weigh the raw materials according to the above weight ratio, add them to the barrel and mix them evenly, heat and melt, and then quickly inject them into the closed tray mold, after the pressure is maintained, injection molding, the mold is taken out and the product is properly trimmed to obtain the ultra-high molecular weight Polyethylene anticorrosive tray.
Embodiment 2
[0027] This embodiment is an ultra-high molecular weight polyethylene anticorrosive tray, which is mainly made of the following parts by weight of raw materials:
[0028] Ultra-high molecular weight polyethylene: 93; polylactic acid: 5.0; polyisobutylene: 0.5; silicone rubber: 0.2; zeolite: 0.5; rheological processing aid potassium fluoride: 0.2; inorganic filler fly ash: 15; and ultra high The molecular weight of molecular weight polyethylene is 5 million.
[0029] The specific preparation method of the tray of this embodiment is the same as that of Embodiment 1, and will not be repeated here.
Embodiment 3
[0031] This embodiment is an ultra-high molecular weight polyethylene anticorrosive tray, which is mainly made of the following parts by weight of raw materials:
[0032] Ultra-high molecular weight polyethylene: 94; polylactic acid: 6.0; polyisobutylene: 0.3; silicone rubber: 0.2; sodium stearate: 0.2; rheological processing aid calcium fluoride: 0.3; inorganic filler titanium dioxide: 20; The molecular weight of high molecular weight polyethylene is 4.1 million.
[0033] The specific preparation method of the tray of this embodiment is the same as that of Embodiment 1, and will not be repeated here.