A kind of high-quality building formwork and preparation method thereof
A technology of building formwork and antimony trioxide, which is applied in the direction of sustainable buildings, can solve problems such as insufficient strength, insufficient heat insulation performance, and insufficient sound insulation performance, and achieve good sound insulation performance, high strength, and improved performance. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0019] A high-quality building template, the raw materials are composed of the following parts by weight: 12 parts of antimony trioxide, 18 parts of ceramic cotton, 20 parts of sodium silicate, 12 parts of ethylene acid, 28 parts of quartz sand, 22 parts of paraffin, 18 parts of sulfomethyl phenolic resin, 16 parts of water glass, 22 parts of calcium pyrophosphate, 18 parts of magnesium bicarbonate, 18 parts of butyl acrylate, 12 parts of tetrabutyl titanate, 14 parts of methyl acetate, 12 parts of titanium oxide and Sodium fluoride 16 parts.
[0020] A method for preparing high-quality building formwork, comprising the following steps:
[0021] 1) Take 12 parts of antimony trioxide, 18 parts of ceramic wool, 20 parts of sodium silicate and 12 parts of ethylene acid, put them into a blender, and stir evenly;
[0022] 2) Put the above-mentioned uniformly stirred materials into the heater, and raise the temperature to 80-100°C for 30-50 minutes, and set aside;
[0023] 3) Take...
Embodiment 2
[0029] A high-quality building template, the raw materials are composed of the following parts by weight: 14 parts of antimony trioxide, 17 parts of ceramic cotton, 19 parts of sodium silicate, 11 parts of ethylene acid, 26 parts of quartz sand, 21 parts of paraffin, 14 parts of sulfomethyl phenolic resin, 14 parts of water glass, 21 parts of calcium pyrophosphate, 15 parts of magnesium bicarbonate, 17 parts of butyl acrylate, 11 parts of tetrabutyl titanate, 13 parts of methyl acetate, 11 parts of titanium oxide and Sodium fluoride 14 parts.
[0030] A method for preparing high-quality building formwork, comprising the following steps:
[0031] 1) Take 14 parts of antimony trioxide, 17 parts of ceramic wool, 19 parts of sodium silicate and 11 parts of ethylene acid, put them into a mixer, and stir evenly;
[0032] 2) Put the above-mentioned uniformly stirred materials into the heater, and raise the temperature to 80-100°C for 30-50 minutes, and set aside;
[0033] 3) Take 2...
Embodiment 3
[0039] A high-quality building template, the raw materials are composed of the following parts by weight: 16 parts of antimony trioxide, 16 parts of ceramic cotton, 18 parts of sodium silicate, 10 parts of ethylene acid, 24 parts of quartz sand, 20 parts of paraffin, 10 parts of sulfomethyl phenolic resin, 12 parts of water glass, 20 parts of calcium pyrophosphate, 12 parts of magnesium bicarbonate, 16 parts of butyl acrylate, 10 parts of tetrabutyl titanate, 12 parts of methyl acetate, 10 parts of titanium oxide and Sodium fluoride 12 parts.
[0040] A method for preparing high-quality building formwork, comprising the following steps:
[0041] 1) Take 16 parts of antimony trioxide, 16 parts of ceramic wool, 18 parts of sodium silicate and 10 parts of ethylene acid, put them into a blender, and stir evenly;
[0042] 2) Put the above-mentioned uniformly stirred materials into the heater, and raise the temperature to 80-100°C for 30-50 minutes, and set aside;
[0043] 3) Take...