Glue for high-temperature stepping motor coil fixation
A stepper motor and coil technology, used in adhesives, epoxy resin glue, non-polymer adhesive additives, etc., can solve problems such as can not be used in vacuum, the motor cannot work, and the coil is short-circuited.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0022] A component is calculated in parts by mass, including the following components: 5 parts of ceramics, 25 parts of E-51 epoxy resin, 20 parts of maleimide, 1 part of asbestos fiber, and 35 parts of ethanol; Counting, including the following components: 75 parts of aromatic amine, 15 parts of molybdenum disulfide.
[0023] Mix the above components A and B according to the mass ratio of 1:1, apply it on one end of the coil, let it stand for 15 minutes, then apply the same amount of glue on the other end and let it stand for 15 minutes, put the motor with the coil on Put it into an incubator at a temperature of 75°C, keep warm for 3.5 hours, and keep turning both ends of the coil up and down at a constant speed while keeping warm.
Embodiment 2
[0025] A component is calculated by mass parts, including the following components: 6 parts of ceramics, 27 parts of E-51 epoxy resin, 23 parts of maleimide, 1.5 parts of asbestos fiber, 38 parts of ethanol; B component by mass parts Counting, including the following components: 78 parts of aromatic amine, 17 parts of molybdenum disulfide.
[0026] Mix the above components A and B according to the mass ratio of 1:1.5, apply it on one end of the coil, let it stand for 20 minutes, then apply the same amount of glue on the other end and let it stand for 20 minutes, put the motor with the coil on Put it into an incubator at a temperature of 80°C, keep warm for 4 hours, and keep turning both ends of the coil up and down at a constant speed while keeping warm.
Embodiment 3
[0028] A component is calculated by mass parts, including the following components: 7 parts of ceramics, 30 parts of E-51 epoxy resin, 25 parts of maleimide, 2 parts of asbestos fiber, 40 parts of ethanol; B component by mass parts Counting, including the following components: 80 parts of aromatic amine, 19 parts of molybdenum disulfide.
[0029] Mix the above components A and B according to the mass ratio of 1:2, apply it on one end of the coil, let it stand for 25 minutes, then apply the same amount of glue on the other end and let it stand for 25 minutes, put the motor with the coil on Put it into an incubator at a temperature of 84°C, keep warm for 4.5 hours, and keep turning both ends of the coil up and down at a constant speed while keeping warm.
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com