Preparation and application of circulating water high-efficiency corrosion and scale inhibitor
A technology of corrosion and scale inhibitor and scale inhibitor, which is applied in the field of circulating water system, can solve the problems of high hardness and alkalinity, and increase the difficulty of purpose, and achieve the effect of saving industrial water and reducing costs.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0011] Embodiment 1: choose raw material by weight percentage:
[0012] HPA 10%
[0013] AMPS 15%
[0014] AA 5%
[0015] Ammonium persulfate 5%
[0016] Sodium hypophosphite 1%
[0017] Pure water 64%
[0018] Add a certain amount of water and reducing agent into a multi-necked flask equipped with a reflux cooler, a thermometer, a constant pressure dropping funnel and a magnetic stirrer, heat up and stir, when the water in the bottle reaches a certain temperature. At the same time, drop the mixed monomer (AA / AMPS, HPA) and oxidant (ammonium persulfate) to maintain a certain temperature range. After the dropwise addition, continue to maintain a certain temperature, keep it warm for a period of time, and cool to obtain the copolymer for corrosion and scale inhibition. agent.
Embodiment 2
[0019] Embodiment 2: select raw material by weight percentage:
[0020] HPA 15%
[0021] AMPS 25%
[0022] AA 10%
[0023] Ammonium persulfate 7%
[0024] Sodium hypophosphite 5%
[0025] Pure water 38%
[0026] Add a certain amount of water and reducing agent into a multi-necked flask equipped with a reflux cooler, a thermometer, a constant pressure dropping funnel and a magnetic stirrer, heat up and stir, when the water in the bottle reaches a certain temperature. At the same time, drop the mixed monomer (AA / AMPS, HPA) and oxidant (ammonium persulfate) to maintain a certain temperature range. After the dropwise addition, continue to maintain a certain temperature, keep it warm for a period of time, and cool to obtain the copolymer for corrosion and scale inhibition. agent.
Embodiment 3
[0027] Embodiment 3: select raw material by weight percentage:
[0028] HPA 20%
[0029] AMPS 30%
[0030] AA 10%
[0031] Ammonium persulfate 10%
[0032] Sodium hypophosphite 5%
[0033] Pure water 25%
[0034] Add a certain amount of water and reducing agent into a multi-necked flask equipped with a reflux cooler, a thermometer, a constant pressure dropping funnel and a magnetic stirrer, heat up and stir, when the water in the bottle reaches a certain temperature. At the same time, drop the mixed monomer (AA / AMPS, HPA) and oxidant (ammonium persulfate) to maintain a certain temperature range. After the dropwise addition, continue to maintain a certain temperature, keep it warm for a period of time, and cool to obtain the copolymer for corrosion and scale inhibition. agent.