[0013] Example 1 A frost-resistant hollow brick, composed of the following raw materials in parts by weight: 37 parts of shale, 1.1 parts of alunite powder, 2.5 parts of sodium pyrophosphate, 8 parts of ordinary portland cement, 7 parts of curing agent, polyethylene 4 parts of rubber powder, 0.08 part of urea, 0.15 part of propylene glycol, 3.5 parts of urea-formaldehyde resin, 4 parts of emulsified asphalt, 2.5 parts of methyl cellulose with a concentration of 3%, and 5 parts of YT inorganic active thermal insulation material.
[0014] Antifreeze hollow brick and preparation method thereof, the specific preparation steps are as follows:
[0015] (1) mechanically pulverize the shale into powder, add the above-mentioned raw materials except the curing agent and stir evenly according to the formula ratio, and then add warm water with a volume ratio of 12-14%;
[0016] (2) add curing agent, then carry out extrusion molding by extrusion equipment;
[0017] (3) Static stopping and...
Embodiment 2
[0018] Example 2 A frost-resistant hollow brick, composed of the following raw materials in parts by weight: 36 parts of shale, 1 part of alum stone powder, 1 part of sodium pyrophosphate, 7 parts of ordinary Portland cement, 6 parts of curing agent, polyethylene 3 parts of rubber powder, 0.05 part of urea, 0.1 part of propylene glycol, 3 parts of urea-formaldehyde resin, 3 parts of emulsified asphalt, 2 parts of methyl cellulose with a concentration of 3%, and 4 parts of YT inorganic active insulation material.
[0019] Antifreeze hollow brick and preparation method thereof, the specific preparation steps are as follows:
[0020] (1) mechanically pulverize the shale into powder, add the above-mentioned raw materials except the curing agent and stir evenly according to the formula ratio, and then add warm water with a volume ratio of 12-14%;
[0021] (2) add curing agent, then carry out extrusion molding by extrusion equipment;
[0022] (3) Static stopping and cutting after f...
Embodiment 3
[0023] Example 3 A frost-resistant hollow brick, composed of the following raw materials in parts by weight: 38 parts of shale, 1.2 parts of alum stone powder, 3 parts of sodium pyrophosphate, 9 parts of ordinary portland cement, 8 parts of curing agent, polyethylene 5 parts of rubber powder, 0.1 part of urea, 0.2 part of propylene glycol, 4 parts of urea-formaldehyde resin, 5 parts of emulsified asphalt, 3 parts of methyl cellulose with a concentration of 3%, and 6 parts of YT inorganic active insulation material.
[0024] Antifreeze hollow brick and preparation method thereof, the specific preparation steps are as follows:
[0025] (1) mechanically pulverize the shale into powder, add the above-mentioned raw materials except the curing agent and stir evenly according to the formula ratio, and then add warm water with a volume ratio of 12-14%;
[0026] (2) add curing agent, then carry out extrusion molding by extrusion equipment;
[0027] (3) Static stopping and cutting afte...
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More