Waterproof and antifreeze impregnating liquid for corrugated cardboard boxes and its preparation and use method
A corrugated box and impregnating liquid technology, which is applied in the direction of papermaking, paper coating, and water-repellent addition, can solve the problems of poor frost resistance and strength, achieve good waterproof and moisture-proof performance, enhance waterproof performance, and ensure uniformity Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0018] A method for preparing a waterproof and antifreeze impregnating liquid for corrugated paper boxes. The preparation method comprises the following steps: mixing and stirring each raw material according to a required ratio at 100-110° C. for 3-5 minutes.
[0019] A method for using a waterproof and antifreeze impregnation solution for corrugated cardboard boxes, the method of use is as follows: first place a corrugated cardboard in the soaking solution at 100-110° C. Dry at 110-130°C, and finally cool at room temperature for more than 20 minutes.
[0020] Principle of the present invention is described as follows:
[0021] The present invention proposes an impregnation solution for corrugated boxes, which can directly form a strong chemical bond with the corrugated box, and quickly solidify on the surface of the corrugated box to form a firm reinforced protective layer, so that even if the corrugated box is placed in low temperature for a long time Its strength will not ...
Embodiment 1
[0037] A waterproof and antifreeze impregnation solution for corrugated boxes, the raw material composition and weight ratio include: paraffin oil 50, EPDM EPDM 10, ethylene-vinyl acetate copolymer EVA 10, thermoplastic acrylic resin 3, vinyl Trimethoxysilane 0.5, nano-scale titanium dioxide 3, jute short fiber 8, wherein the thermoplastic acrylic resin is polymerized from n-butyl methacrylate monomer.
[0038] The preparation method of the above-mentioned waterproof and antifreeze impregnation solution for corrugated cardboard boxes is as follows: adding the above-mentioned raw materials into the impregnation tank according to the required ratio, and mixing and stirring at 100° C. for 5 minutes.
[0039] The method of using the above-mentioned waterproof and antifreeze impregnating solution for corrugated cardboard boxes is as follows: first, use the automatic cardboard feeding machine to send the corrugated cardboard into the dipping tank filled with the dipping solution at 1...
Embodiment 2
[0041] Step is with embodiment 1, and difference is:
[0042] The raw material composition and weight ratio of the waterproof and antifreeze dipping solution for corrugated boxes are: paraffin oil 70, EPDM EPDM 15, ethylene-vinyl acetate copolymer EVA 15, thermoplastic acrylic resin 5, vinyl trimethyl Oxysilane 0.8, nanoscale titanium dioxide 5, jute short fiber 10.
[0043] In the preparation method of the waterproof and antifreeze impregnation solution for corrugated cardboard boxes, the mixing temperature is 110° C., and the mixing time is 3 minutes.
[0044] In the method for using the waterproof and antifreeze dipping solution for corrugated cardboard boxes, the temperature of the dipping solution is 110°C, the dipping time is 5s, the temperature in the hot air chamber is 130°C, the moving speed of the corrugated cardboard is 15m / min, and the cooling time is 30min .
PUM
| Property | Measurement | Unit |
|---|---|---|