A heavy-duty anti-corrosion high-memory microfiber armor
A heavy-duty anti-corrosion and memory fiber technology, which is applied to the anti-corrosion of metal structures, concrete, and wood, can solve the problems of serious safety hazards, high prices, and inconvenient construction, etc., to block the intrusion of corrosive media and excellent anti-corrosion performance , Excellent anti-corrosion effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
specific Embodiment approach 1
[0049] 1.2-meter-diameter offshore wharf steel pipe pile protection with a protection length of 3.5 meters.
[0050] The operation steps are as follows:
[0051] S1: The length of the cut microfiber armor is 3.5 meters, and the width is 3.5 meters. The microfiber armor specifically includes: high-strength protective outer layer 1, high-memory fiber layer 2, buffer protection layer 3, and solid oil layer 4.
[0052] The high-strength protective outer layer 1 is set as one layer, the high-memory fiber layer 2 is set as one layer, the buffer protection layer 3 is set as one layer, and the solid oil layer 4 is set as one layer.
[0053] S2: Use a shovel to remove marine organisms, poorly attached old coatings, and rust layers on the surface of steel pipe piles.
[0054] S3: Unfold the microfiber armor, wrap it in the protected area of the steel pipe pile, and fix it with 12 high-strength polymer binding straps 7 . The distance between every two binding straps is 30cm.
specific Embodiment approach 2
[0055] Anti-corrosion protection of steel piles for offshore wind power foundations with a diameter of 5 meters and a protection length of 6 meters.
[0056] The operation steps are as follows:
[0057] S1: The length of the cut microfiber armor is 14.5 meters. There are 8 pieces of the microfiber armor, of which 4 pieces are 3.2 meters wide and 4 pieces are 3.0 meters wide.
[0058] The microfiber armor is double-layered, and the structure includes: a high-strength protective outer layer 13, a double-layer high-memory fiber layer 23, a double-layer buffer protection layer 33, and a solid oil layer 4.
[0059] Wherein the high-strength protective outer layer 1 is set as 1 layer, the high-memory fiber layer 2 is set as 2 layers, the buffer protection layer 3 is set as 2 layers, and the solid oil layer 4 is set as 1 layer, wherein the solid oil layer 4 is completely soaked with anti-corrosion petrolatum.
[0060] S2: Use a high-pressure water gun to remove marine organisms, wea...
specific Embodiment approach 3
[0062] The side length is 0.5 meters and the square marine reinforced concrete pile is protected, and the protection length is 3.5 meters.
[0063] The operation steps are as follows:
[0064] S1: The cut microfiber armor has a length of 1.85 meters and a width of 3.5 meters. The microfiber armor includes: a high-strength protective outer layer 1, a high memory enhancement layer 2, a buffer protection layer 3, a solid oil layer 4, and a sacrificial anode layer 5.
[0065] Among them, the high-strength protective outer layer 1 is set to 1 layer, the high memory enhancement layer 2 is set to 1 layer, the buffer protection layer 3 is set to 1 layer, the solid oil layer 4 is set to 1 layer, and the aluminum alloy sacrificial anode layer 5 is set to 1 layer. Armor Flange 6 stitched in two sections.
[0066] S2: Use high-pressure water to remove the attachments on the pile surface and the loose concrete layer.
[0067] S3: Unfold the microfiber armor, wrap it around the pile prot...
PUM
| Property | Measurement | Unit |
|---|---|---|
| thickness | aaaaa | aaaaa |
| thickness | aaaaa | aaaaa |
| thickness | aaaaa | aaaaa |