An odor and advertising technology, applied in the field of anti-snow odor advertising materials, can solve the problems of easily damaged advertising materials, shortening the service life, blocking the line of sight, etc., to achieve the effect of being conducive to promotion and application, convenient production, and not easy to freeze
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0030] Further, the anti-snow odor advertising material is prepared by the following method:
[0031] a. Weigh the material, mix the product essence, slow-release agent and antifreeze to obtain mixture A;
[0032] b. Mix polyethylene and polyacrylamide;
[0033] c. mix calcium carbonate and ethyl cellulose;
[0034] d. Mix paraffin, acetic acid, attapulgite, graphite, potassium nitrate, ice crystal sand, and calcium chloride evenly to obtain a mixture D energy storage material;
[0035] e. Mix the materials mixed in steps b and c, and the antifreeze agent at 100-110°C for 5-8 minutes, add mixture D and foaming agent, and mix at 120-140°C for 8-8 minutes After 12 minutes, cool to 80-85°C, add mixture A, keep at 80-85°C, 0.5-0.6Mpa for 15-20 minutes to obtain snow-proof advertising material.
[0036] The technology of the preparation method of snow-proof smell advertisement material of the present invention is as follows:
[0037] a. Weigh the material, mix the product essen...
Embodiment 1
[0043] Take 0.2 g of 2,2,2-nitrosotriethanol, 0.12 g of sodium nitrate, 0.08 g of benzotriazole amine salt, and 120 g of ethylene glycol and mix them to obtain an antifreeze agent.
[0044] Take by weighing 80 parts by weight of polyethylene, 20 parts by weight of mango essence, 25 parts by weight of polyethylene glycol, 8 parts by weight of calcium carbonate, 4 parts by weight of polyacrylamide, 4 parts by weight of ethyl cellulose, 5 parts by weight of antifreeze, 1 part by weight of cyclopentane, 6 parts by weight of paraffin, 6 parts by weight of acetic acid, 3 parts by weight of attapulgite, 3 parts by weight of graphite, 3 parts by weight of potassium nitrate, 7 parts by weight of ice crystal sand, and 4 parts by weight of calcium chloride.
[0045] a. Mango essence, polyethylene glycol and antifreeze are mixed to obtain mixture A;
[0046] b. Mix polyethylene and polyacrylamide;
[0047] c. mix calcium carbonate and ethyl cellulose;
[0048] d. Mix paraffin, acetic ac...
Embodiment 2
[0051] Take 0.2 g of 2,2,2-nitrosotriethanol, 0.12 g of sodium nitrate, 0.08 g of benzotriazole amine salt, and 120 g of ethylene glycol and mix them to obtain an antifreeze agent.
[0052] Take by weighing 85 parts by weight of polyethylene, 20 parts by weight of jasmine essence, 20 parts by weight of polyethylene glycol, 10 parts by weight of guar gum, 5 parts by weight of calcium carbonate, 3 parts by weight of polyacrylamide, 4 parts by weight of ethyl cellulose, 5 parts by weight of antifreeze, 1 part by weight of isopentane, 8 parts by weight of paraffin, 8 parts by weight of acetic acid, 4 parts by weight of attapulgite, 3 parts by weight of graphite, 4 parts by weight of potassium nitrate, 8 parts by weight of ice crystal sand, chlorinated 5 parts by weight of calcium.
[0053] a. jasmine essence, polyethylene glycol, guar gum and antifreeze are mixed to obtain mixture A;
[0054] b. Mix polyethylene and polyacrylamide;