[0023] Embodiment 1: a kind of method utilizing plant glue to prepare sealing ring,
[0024] Take 100 parts of soybean protein, isolate protein 8%-20% from soybean, urea 15%-17%, sodium polyphosphate 1%-10%, disperse urea in water, mix to make urea solution, add protein and mixture , stirred at room temperature for 1-2 hours, then added 5 parts of turpentine, continued to stir for 2-3 hours, and finally added 15 parts of 50% sodium hydroxide aqueous solution, stirred at high temperature for 20 minutes, and controlled the temperature at 90-95°C;
[0025] Slowly add 30 parts of water glass and 2 parts of thiourea under the action of stirring and / or ultrasound, and react at a temperature of 0-80°C for 0.1-12 hours. dry;
[0026] Mix the dried granules with 15 parts of 20% sodium carbonate aqueous solution, beat, add 15 parts of 50% sodium hydroxide aqueous solution and 100 parts of water, heat, add 30 parts of epoxy resin after 20 minutes, and refine for 2 hours. get the glue; ...
Embodiment 2
[0042] Embodiment 2: a kind of method utilizing vegetable glue to prepare sealing ring,
[0043] Take 120 parts of soybean protein, isolate protein 8%-20% from soybean, urea 15%-17%, sodium polyphosphate 1%-10%, disperse urea in water, mix to make urea solution, add protein and mixture , stirred at room temperature for 1-2 hours, then added 7 parts of turpentine, continued to stir for 2-3 hours, and finally added 20 parts of 50% sodium hydroxide aqueous solution, stirred at high temperature for 20 minutes, and controlled the temperature at 90-95 °C;
[0044] Slowly add 40 parts of water glass and 5 parts of thiourea under stirring and / or ultrasonic action, and react at a temperature of 0-80°C for 0.1-12 hours. dry;
[0045] Mix the dry granules with 20 parts of 20% sodium carbonate aqueous solution, beat, add 20 parts of 50% sodium hydroxide aqueous solution and 130 parts of water, heat, add 50 parts of epoxy resin after 20 minutes, and refine for 2 hours. get the glue;
[...