Gypsum board capable of inducing anions and preparation method of gypsum board
A technology of gypsum board and negative ions, which is applied in the field of building materials, can solve the problems of large tourmaline content, human injury, and large resource consumption, and achieve the effects of low production and preparation costs, reduced radioactivity, and improved induction effects
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0023] (1) Take 60% of gypsum board raw material by mass percentage, 16% of nano-tourmaline, 8% of nano-titanium dioxide, 8% of superfine calcium hardate, 8% of superfine talcum powder, and mix them into powder;
[0024] (2) The mass ratio of powder and water is mixed according to 7:3, and stirred for 10 minutes until a uniform slurry is formed;
[0025] (3) Flow the uniformly stirred slurry into the belt, and the conveying roller presses the slurry to form itself;
[0026] (4) The formed product is first cured at room temperature for 6 hours, then autoclaved at 100°C for 10 hours, and finally baked at 100°C for 6 hours.
[0027] A gypsum board that induces negative ions can be prepared.
Embodiment 2
[0029] (1) Take gypsum board raw material 65%, nano tourmaline 12.5%, nano titanium dioxide 7.5%, ultrafine calcium hardate 7.5%, ultrafine talcum powder 7.5% by mass percentage, mix into powder;
[0030] (2) The mass ratio of powder and water is mixed according to 7:3, and stirred for 10 minutes until a uniform slurry is formed;
[0031] (3) Flow the uniformly stirred slurry into the belt, and the conveying roller presses the slurry to form itself;
[0032] (4) The formed product is first cured at room temperature for 8 hours, then autoclaved at 80°C for 12 hours, and finally baked at 120°C for 5 hours.
[0033] A gypsum board that induces negative ions can be prepared.