A kind of spiral burr type aluminum alloy cylinder liner and preparation method thereof
An aluminum alloy, helical technology, applied in the field of helical burr-type aluminum alloy cylinder liner and its preparation, can solve the difficulty in meeting the requirements of cylinder liner strength, wear resistance and cost, low yield and productivity, and cylinder liner production High cost and other problems, to achieve the effect of shortening the running-in time, prolonging the service life and improving the bonding strength
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0026] Such as figure 1 As shown, this embodiment discloses a helical burr-type aluminum alloy cylinder liner, a helical burr-type aluminum alloy cylinder liner, including a cylinder liner body, the inner surface of the cylinder liner body is coated with an inner coating 1, the The surface roughness of the inner coating 1 is 80 μm, and the thickness is 0.2 mm; the outer surface of the cylinder liner body is provided with burrs 11, which are distributed in a spiral shape, and the height of the burrs 11 is 0.1 mm.
[0027] The chemical composition of the cylinder liner body includes Si content of 5wt.%, Ti content of 7wt.%, Fe content of 0.3wt.%, Mn content of 0.6wt.%, Pd content of 0.05wt.%. The Sr content is 2.3wt.%, and the rest is Al.
Embodiment 2
[0029] Such as figure 1 As shown, this embodiment discloses a spiral burr-type aluminum alloy cylinder liner, including a cylinder liner body, the inner surface of the cylinder liner body is coated with an inner coating 1, and the surface roughness of the inner coating 1 is 100 μm , the thickness is 0.3mm; the outer surface of the cylinder liner body is provided with burrs 11, and the burrs 11 are distributed in a spiral shape, and the height of the burrs 11 is 0.3mm. The chemical composition of the cylinder liner body includes Si content of 5wt.%, Ti content of 7~8wt.%, Fe content of 0.35wt.%, Mn content of 0.7wt.%, Pd content of 0.06wt. %, the Sr content is 2.5wt.%, and the rest is Al.
Embodiment 3
[0031] Such as figure 1 As shown, this embodiment discloses a spiral burr-type aluminum alloy cylinder liner, including a cylinder liner body, the inner surface of the cylinder liner body is coated with an inner coating 1, and the surface roughness of the inner coating 1 is 80 ~120 μm, the thickness is 0.2~0.4mm; the outer surface of the cylinder liner body is provided with burrs 11, the burrs 11 are distributed in a spiral shape, and the height of the burrs 11 is 0.1~0.5mm.
[0032] The chemical composition of the cylinder liner body includes Si content of 6wt.%, Ti content of 8wt.%, Fe content of 0.4wt.%, Mn content of 0.8wt.%, Pd content of 0.07wt.%. The Sr content is 2.6wt.%, and the rest is Al.
[0033] Since the inner coating of the invention is attached to the inner surface of the cylinder liner body and has relatively high hardness, the running-in time of the cylinder liner can be shortened and the service life of the cylinder liner can be prolonged. The thickness of...
PUM
Property | Measurement | Unit |
---|---|---|
surface roughness | aaaaa | aaaaa |
thickness | aaaaa | aaaaa |
height | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com