Environment-friendly adhesive glue special for decoration and preparation method thereof
A kind of bonding glue, environmental protection technology, applied in the direction of epoxy resin glue, adhesive, adhesive type, etc., can solve unfavorable health and other problems, and achieve the effect of short curing time, high viscosity and long service life
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0012] A special environment-friendly adhesive for decoration and a preparation method thereof. The raw materials are composed of the following proportions in parts by weight: 16 parts of epoxy resin, 4 parts of polyvinyl chloride resin, 4 parts of polypropylene resin, 12 parts of terpene resin, Dioctyl phthalate 13 parts, polyorganosiloxane 7 parts, simethicone 6 parts, potassium sorbate 5 parts, white carbon black 3 parts, ethanol 35 parts.
[0013] Its preparation method is as follows:
[0014] A. Copolymerize epoxy resin, polyvinyl chloride resin and terpene resin, set the pressure at 290°C, set the pressure at 0.8MPa, use white carbon black as the catalyst, add polypropylene resin after 15 minutes for melting, mixing and stirring, and stir The speed is 500r / min, and the mixture A is obtained after stirring evenly;
[0015] B. Add dioctyl phthalate, polyorganosiloxane and dimethyl silicone oil into ethanol for dissolution, and use ultrasonic treatment at a frequency of 60...
Embodiment 2
[0018] A special environment-friendly adhesive for decoration and a preparation method thereof. The raw materials are composed of the following proportions in parts by weight: 20 parts of epoxy resin, 3 parts of polyvinyl chloride resin, 5 parts of polypropylene resin, 8 parts of terpene resin, Dioctyl phthalate 15 parts, polyorganosiloxane 4 parts, simethicone 8 parts, potassium sorbate 3 parts, white carbon black 5 parts, ethanol 30 parts.
[0019] Its preparation method is as follows:
[0020] A. Copolymerize epoxy resin, polyvinyl chloride resin and terpene resin, set the pressure at 320°C, set the pressure at 0.8MPa, use white carbon black as the catalyst, add polypropylene resin after 15 minutes for melting, mixing and stirring, and stir The speed is 450r / min, and the mixture A is obtained after stirring evenly;
[0021] B. Add dioctyl phthalate, polyorganosiloxane and dimethyl silicone oil into ethanol for dissolution, and use ultrasonic treatment with a frequency of 6...
Embodiment 3
[0024] A special environment-friendly adhesive for decoration and a preparation method thereof. The raw materials are composed of the following proportions in parts by weight: 15 parts of epoxy resin, 5 parts of polyvinyl chloride resin, 3 parts of polypropylene resin, 15 parts of terpene resin, Dioctyl phthalate 10 parts, polyorganosiloxane 8 parts, simethicone 5 parts, potassium sorbate 6 parts, white carbon black 3 parts, ethanol 45 parts.
[0025] Its preparation method is as follows:
[0026] A. Copolymerize epoxy resin, polyvinyl chloride resin and terpene resin, set the pressure at 320°C, set the pressure at 0.9MPa, use white carbon black as the catalyst, add polypropylene resin after 10 minutes for melting, mixing and stirring, and stir The speed is 550r / min, and the mixture A is obtained after stirring evenly;
[0027] B. Add dioctyl phthalate, polyorganosiloxane and dimethyl silicone oil into ethanol for dissolution, and use ultrasonic treatment with a frequency of ...