Profile controlling and flooding for weak gel complex clay and preparation method thereof
A technology of control and displacement agent and weak gel, which is applied in the field of control and displacement agent of weak gel compound clay and its preparation, can solve the problems of short action time, low control and displacement intensity, difficulty in deep oil well control and displacement, and achieve Long action time, high control and flooding intensity, and the effect of increasing oil recovery by water flooding
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0030] In the second aspect, the embodiment of the present invention provides a preparation method of the above-mentioned drive control agent, the preparation method comprising the following steps:
[0031] Step 101. According to the parts by weight of the components in the water-displacing agent, add clear water into the jar, then add polyacrylamide under stirring conditions, continue stirring, and then ripen for 7-9 hours to obtain a polyacrylamide solution.
[0032] Step 102: Add clay into the polyacrylamide solution under stirring, and continue stirring to obtain a polyacrylamide-clay mixed system.
[0033] Step 103, adding a basic conditioner to the polyacrylamide-clay mixing system, stirring evenly, then adding a crosslinking agent, stirring evenly again, to obtain a regulating and displacing agent for weak gel compound clay.
[0034] The preparation method of the regulating and displacing agent of the above-mentioned weak gel compound clay provided in the embodiment of ...
Embodiment 1
[0042] This embodiment provides a kind of adjusting and displacing agent of weak gel compound clay, which is prepared by the following method: add 100 parts by weight of clear water to a jar, and then mix 0.05 parts by weight of Add polyacrylamide into the jar, stir for 2 hours, mature for 8 hours, then add 0.1 parts by weight of clay into the jar, stir for 20 minutes, then add 0.001 parts by weight of sodium hydroxide into the jar, stir evenly, and finally Add 0.05 parts by weight of chromium acetate into the jar, and stir evenly to obtain the regulating and displacing agent for weak gel compound clay provided in this example.
[0043] Wherein, the mesh number of the clay is 250 mesh, and the mass percentage of each component in the clay is 80% of montmorillonite, 15% of kaolinite, and the balance of unavoidable impurities.
Embodiment 2
[0045] This embodiment provides a kind of adjusting and displacing agent of weak gel compound clay, which is prepared by the following method: add 100 parts by weight of clear water to a jar, and then mix 0.04 parts by weight of Add polyacrylamide into the jar, stir for 2.1 hours, mature for 9 hours, then add 0.12 parts by weight of clay into the jar, stir for 22 minutes, then add 0.002 parts by weight of sodium hydroxide and sodium carbonate to the jar Stir the mixture evenly, and finally add 0.06 parts by weight of chromium acetate into the jar, and stir evenly to obtain the regulating and displacing agent for weak gel compound clay provided in this example.
[0046] Wherein, the mesh number of clay is 270 meshes, and the mass percent component of each composition in clay is montmorillonite 70%, kaolinite 15%, and the unavoidable impurity of remainder, the mass ratio of sodium hydroxide and sodium carbonate 1:1.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com