A technology of fiber particles and filter paper, applied in the direction of filter paper, filtration separation, separation methods, etc., can solve the problems of poor degradation performance, large air resistance, poor particle filtration efficiency, etc., and achieve low cost, good air permeability, and high filtration accuracy Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0040] The preparation method of air particle filter paper comprises the following steps:
[0041] Step (1): Prepare materials
[0042] The rush core fiber particles: take 65-75 parts of the rush core, grind it to 0.5-1mm with a grinder, and set aside;
[0043] Wood pulp fiber: Take 15-25 parts of wood pulp fiber, dissolve in 500-1000 parts of water, and set aside;
[0044] Amylopectin: take 5-10 parts of amylopectin and set aside;
[0045] Step (2): Plasma knocking
[0046] Mix the above-mentioned rush core fiber particles and wood pulp fibers, add 900-1100 parts of water, beat with a beater for 5 minutes, stop for 2 minutes, and then beat for 5 minutes until there are no pulp lumps, and when the dispersion is uniform, stop beating, and then add the above-mentioned pullulan As a retention aid, stir for 1 minute to obtain a liquid slurry;
[0047] Step (3): Press paper
[0048] Pour the liquid slurry obtained in step (2) into a material basin with a 2mm stainless steel fl...
example 1
[0056] Step (1): Prepare materials
[0057] Rush core fiber particles: take 75g of rush core, grind it to 0.5-1mm with a grinder, and set aside;
[0058] Wood pulp fiber: take 15g of wood pulp fiberboard;
[0059] Amylopectin: take 10g of amylopectin and set aside;
[0060] Step (2): Plasma knocking
[0061] Add 900g of water to the wood pulp fiberboard, beat it with dissolving pulp for 5 minutes, and stop for 2 minutes; then knock it for 5 minutes, and after 1 hour, stop beating until there are no pulp lumps and the dispersion is uniform;
[0062] Step (3): Mixing Knocking
[0063] Add the rush core particles into the kneaded wood pulp, and continue knocking for 30 minutes, until the wood pulp fibers are decomposed and melted, and form a link with the rush core particles to form a suspension;
[0064] Step (4) adds above-mentioned 10g pullulan as retention aid again, stirs 1 minute, obtains liquid slurry;
[0065] Step (5): Papermaking and pressing
[0066] Pour the liq...
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
particle diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com