A pavement brick and noise reduction technology, applied in the field of pavement bricks, can solve the problems of local waterlogging, low strength, endangering road traffic safety, etc., achieve the effect of large pores, improve toughness and compression resistance, and improve toughness and wear resistance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0027] This embodiment relates to a pavement brick with sound-absorbing and noise-reducing functions, including the following raw materials in parts by weight: 10 parts of vermiculite, 15 parts of expanded perlite, 20 parts of modified light calcium carbonate, 18 parts of cement, and 13 parts of silica fume , 6 parts of barite powder, 4 parts of muscovite, 7 parts of shale rock, 3 parts of tourmaline powder, 2 parts of nano-titanium dioxide, 3 parts of polypropylene fiber, 1 part of cellulose ether, 1 part of dispersant, and 2 parts of binder.
[0028] Wherein, the preparation method of described modified light calcium carbonate is as follows:
[0029] Dilute the coupling agent with 5 times the weight of the coupling agent xylene as a solvent, then evenly disperse it in the calcium carbonate, completely volatilize the xylene through an oven, and then grind the dried calcium carbonate into fine powder with a pulverizer to prepare Modified calcium carbonate was obtained.
[003...
Embodiment 2
[0040] This embodiment relates to a pavement brick with sound-absorbing and noise-reducing functions, including the following raw materials in parts by weight: 20 parts of vermiculite, 25 parts of expanded perlite, 30 parts of modified light calcium carbonate, 27 parts of cement, and 19 parts of silica fume , 12 parts of barite powder, 7 parts of muscovite, 11 parts of shale rock, 5 parts of tourmaline powder, 4 parts of nano-titanium dioxide, 8 parts of polypropylene fiber, 2 parts of cellulose ether, 3 parts of dispersant, and 4 parts of binder.
[0041] Wherein, the preparation method of described modified light calcium carbonate is as follows:
[0042] Dilute the coupling agent with 5 times the weight of the coupling agent xylene as a solvent, then evenly disperse it in the calcium carbonate, completely volatilize the xylene through an oven, and then grind the dried calcium carbonate into fine powder with a pulverizer to prepare Modified calcium carbonate was obtained.
...
Embodiment 3
[0053] This embodiment relates to a pavement brick with sound-absorbing and noise-reducing functions, including the following raw materials in parts by weight: 12 parts of vermiculite, 17 parts of expanded perlite, 24 parts of modified light calcium carbonate, 20 parts of cement, and 15 parts of silica fume , 8 parts of barite powder, 5 parts of muscovite, 8 parts of shale rock, 3.6 parts of tourmaline powder, 2.5 parts of nano-titanium dioxide, 4 parts of polypropylene fiber, 1.2 parts of cellulose ether, 1.5 parts of dispersant, and 2.4 parts of binder.
[0054] Wherein, the preparation method of described modified light calcium carbonate is as follows:
[0055] Dilute the coupling agent with 5 times the weight of the coupling agent xylene as a solvent, then evenly disperse it in the calcium carbonate, completely volatilize the xylene through an oven, and then grind the dried calcium carbonate into fine powder with a pulverizer to prepare Modified calcium carbonate was obtai...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com