Sepiolite adsorption facial cleanser and preparing method thereof
A technology of meerschaum and facial cleanser, which is applied in the field of skin care cosmetics, can solve the problems of poor adsorption capacity and killing bacteria, and achieve the effect of promoting absorption, high active ingredients and rich nutrition
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0030] A sepiolite adsorption facial cleanser, which is composed of the following raw materials in parts by weight: 4 parts of submicron modified sepiolite, 6 parts of snail mucus extract, 12 parts of aloe extract, 16 parts of milk, 3 parts of lemon juice, olive Oil 3 parts, camellia oil 5 parts, stearic acid 2 parts, polyethylene glycol 6 parts, pearl powder 4 parts, deionized water 50 parts.
[0031] The preparation method of described submicron modified sepiolite is:
[0032] a. Purification: using layered chain silicate clay mineral sepiolite as raw material, after pounding, slurry treatment, screening, precipitation to remove impurities, dehydration and washing, then drying and crushing, purified sepiolite is obtained. Its sepiolite content is 98%, and its particle size is 0.1 μm;
[0033] b. Modification: the purified sepiolite is subjected to heat treatment, and the temperature is controlled at 550° C. to obtain submicron modified sepiolite.
[0034] The preparation m...
Embodiment 2
[0044] A sepiolite adsorption facial cleanser, which is composed of the following raw materials in parts by weight: 5 parts of submicron modified sepiolite, 7 parts of snail mucus extract, 13 parts of aloe extract, 17 parts of milk, 3.5 parts of lemon juice, olive 4 parts of oil, 6 parts of camellia oil, 2.5 parts of stearic acid, 6.2 parts of polyethylene glycol, 4.6 parts of pearl powder, and 52 parts of deionized water.
[0045] The preparation method of described submicron modified sepiolite is:
[0046]a. Purification: using layered chain silicate clay mineral sepiolite as raw material, after pounding, slurry treatment, screening, precipitation to remove impurities, dehydration and washing, then drying and crushing, purified sepiolite is obtained. Its sepiolite content is 99%, and its particle size is 0.1 μm;
[0047] b. Modification: the purified sepiolite is subjected to heat treatment, and the temperature is controlled at 580° C. to obtain submicron modified sepiolite...
Embodiment 3
[0058] A sepiolite adsorption facial cleanser, which consists of the following raw materials in parts by weight: 6 parts of submicron modified sepiolite, 8 parts of snail mucus extract, 14 parts of aloe extract, 18 parts of milk, 4 parts of lemon juice, olive 4.5 parts of oil, 7 parts of camellia oil, 3 parts of stearic acid, 7 parts of polyethylene glycol, 5 parts of pearl powder, and 55 parts of deionized water.
[0059] The preparation method of described submicron modified sepiolite is:
[0060] a. Purification: using layered chain silicate clay mineral sepiolite as raw material, after pounding, slurry treatment, screening, precipitation to remove impurities, dehydration and washing, then drying and crushing, purified sepiolite is obtained. Its sepiolite content is 99%, and its particle size is 0.2μm;
[0061] b. Modification: the purified sepiolite is subjected to heat treatment, and the temperature is controlled at 600° C. to obtain submicron modified sepiolite.
[006...
PUM
Property | Measurement | Unit |
---|---|---|
Granularity | aaaaa | aaaaa |
Granularity | aaaaa | aaaaa |
Granularity | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com