A technology of optical reflection and reflective coating, which is applied in the field of optoelectronic materials, can solve the problems affecting the visual effect of the backlight panel and the optical quality of the backlight panel, and achieve the effect of reducing impact, reducing friction and high density
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0022] Embodiment 1: an optical reflective sheet, including a base material and a reflective coating, the base material is a polycarbonate polymer, and the mass percentage of the raw material of the reflective coating is: diol diacrylate 65%, Trifluorooxymethacrylate 3%, silica sol 7%, fluorosilane 5%, photoinitiator 3%, calcium carbonate 0.5%, sulfuric acid 0.5%, ethanol 0.5%, ammonia 0.5%, deionized water quantity.
[0023] The preparation method of the above-mentioned optical reflection sheet and its emissive coating comprises the following steps:
[0024] (1) According to the formula of reflective coating, take quantitative trifluorooxymethacrylate, silica sol, fluorosilane, photoinitiator, calcium carbonate, sulfuric acid, ethanol, ammoniacal liquor and deionized water, and will It is stirred and mixed, and diol diacrylate is slowly added under the stirring state, and left to stand after stirring for 4 hours.
[0025] (2) Sintering the reflective coating that has been l...
Embodiment 2
[0027] Embodiment 2: A preparation method of an optical reflective sheet and its emissive coating, including a base material and a reflective coating, the base material is a polycarbonate polymer, and the mass percentage of the raw material of the reflective coating is: two Alcohol diacrylate 70%, trifluorooxymethacrylate 2%, silica sol 4%, fluorosilane 4%, photoinitiator 3%, calcium carbonate 0.2%, sulfuric acid 0.3%, ethanol 0.3%, ammonia water 0.3%, the balance in deionized water. The preparation method is the same as in Example 1.
Embodiment 3
[0028] Embodiment 3: An optical reflective sheet and its emissive coating preparation method, including a base material and a reflective coating, the base material is polycarbonate polymer, and the raw material mass percentage of the reflective coating is: two Alcohol diacrylate 60%, trifluorooxymethacrylate 5%, silica sol 9%, fluorosilane 6%, photoinitiator 5%, calcium carbonate 0.5%, sulfuric acid 0.4%, ethanol 0.5%, ammonia water 0.5%, the balance in deionized water. The preparation method is the same as in Example 1.