Process for producing low-weight high-strength corrugated paper on high-speed paper machine
A high-speed paper machine and low basis weight technology, applied in the field of papermaking, can solve the problems of charge balance damage, high production system requirements, and increased waste water, and achieve the effects of improving fine fibers, reducing operational obstacles, and avoiding negative effects
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0033] A process for producing low-quantity high-strength corrugated paper on a high-speed paper machine, wherein the specific steps of the process are as follows:
[0034] 1. Waste cartons are drum pulped and enter the flotation cell. Add fatty acid sodium deinking agent according to the amount of 1.5kg / ton of waste paper, and remove large stickies and light and heavy materials through coarse sieve, fine sieve and desander. Impurities, the purified slurry is then passed through a thermal dispersion refiner. After the above process, the quality of the waste paper pulp slurry: ash content 18%; whiteness 38% ISO; pH value 7.1; sticky matter content 880mm 2 / kg;
[0035] 2. Polyvinyl alcohol fibers are selected from polyvinyl alcohol fibers with a melting temperature of 45 degrees, and the length is 6mm. The polyvinyl alcohol fibers are decomposed and dispersed evenly in a hydropulper at a concentration of 3-5%, and the temperature of the water is not higher than 45 degrees. Spe...
Embodiment 2
[0045] A process for producing low-quantity high-strength corrugated paper on a high-speed paper machine, wherein the specific steps of the process are as follows:
[0046] 1. The waste cartons are pulped by a drum, and then enter the flotation tank, add 3kg / ton of waste paper, add fatty acid sodium deinking agent, and remove large stickies and light and heavy impurities through coarse sieves, fine sieves, and desanders. The purified pulp is then passed through a thermal dispersion refiner. After the above process, the quality of the waste paper pulp pulp is as follows: ash content 14%; whiteness 42% ISO; pH value 7.5; sticky matter content 650mm 2 / kg;
[0047] 2. Polyvinyl alcohol fibers are selected from polyvinyl alcohol fibers with a melting temperature of 65 degrees and a length of 3mm. The polyvinyl alcohol fibers are decomposed and dispersed evenly in a hydropulper at a concentration of 3-5%, and the temperature of the water is not higher than 45 Spend. In the mixed ...
PUM
Property | Measurement | Unit |
---|---|---|
Length | aaaaa | aaaaa |
Length | aaaaa | aaaaa |
Length | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com