Flow guide ring casting numerical control machining mold and manufacturing method thereof
A technology for processing molds and manufacturing methods, which is applied in the field of CNC machining molds for diversion ring castings and its manufacturing, and can solve the problem of poor product strength, wear resistance, adhesion, surface gloss and non-deformation, which are difficult to guarantee Problems such as the glossiness of the product surface and the difficulty of CNC machine tools, etc., to achieve the effect of surface coating treatment, smooth and delicate product surface, and improve surface quality
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0041] When the production temperature is 0°C-15°C, the skin covering layer includes the following raw materials in parts by weight: 30 parts, 15 parts, and 55 parts of industrial brine.
[0042] A method for manufacturing a numerical control machining mold for a diversion ring casting, comprising the steps of:
[0043] 1) According to the processing workpiece, make a timber frame;
[0044] 2) According to the above-mentioned parts by weight, the skin covering raw materials are evenly mixed, and then the wood frame is covered and molded, compacted, dried and solidified, and the initial processing mold is obtained;
[0045] For the part where the fillet of the product is above 15°, combined with the above temperature, fossil powder is added to the skin covering raw material formula in proportion, and the addition ratio is skin covering material: talcum powder = 4:1, and the amount of talc powder added is 25 parts;
[0046] 3) According to the product size and precision requireme...
Embodiment 2
[0050] When 5°C
[0051] A method for manufacturing a numerical control machining mold for a diversion ring casting, comprising the steps of:
[0052] 1) According to the processing workpiece, make a timber frame;
[0053] 2) According to the above-mentioned parts by weight, the skin covering raw materials are evenly mixed, and then the wood frame is covered and molded, compacted, dried and solidified, and the initial processing mold is obtained;
[0054] For the part where the fillet of the product is above 15°, combined with the above temperature, fossil powder is added to the skin covering raw material formula in proportion, and the addition ratio is skin covering material: talc powder = 5:1, and the amount of talc powder added is 20 parts;
[0055] 3) According to the product size and precision requirements, carry ...