A compound grinding and pelletizing technology, applied in chemical instruments and methods, mixers, dissolving, etc., can solve the problems of uneven uniformity, high investment in wet grinding, and difficult control of discharge moisture, and achieves improved quality and grade, The effect of maximizing grinding efficiency and saving consumption
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0047] Pellet compound grinding and batching scheme, see Table 1 for details:
[0048] Table 1 pellet grinding and batching scheme, % (mass percentage)
[0049]
[0050] In Table 1, Ig refers to burning loss, if the iron ore powder is magnetite, that is, the FeO content is very high, then it will be oxidized and weighted during the roasting process, and the final burning loss is reflected as a negative number (such as burning loss "-2.2%" , "-2.3%").
[0051] The process of pellet compound grinding is as follows: dry-grind iron ore powder A (the amount used is 50% of the total mass of iron ore powder), and the proportion of 0-8mm before grinding accounts for 91%, and it forms 0-200 mesh after grinding. Accounting for 90% of the finished product, the moisture before grinding is 8.5%, and the moisture after grinding is 2.0%. The iron ore powder B (the amount used is 50% of the total mass of iron ore powder) is wet-milled, and the proportion from 0-8mm before grinding account...
example 2
[0054] Table 2 pellet grinding and batching scheme, % (mass percentage)
[0055]
[0056] A pelletizing compound grinding system and a pelletizing compound grinding method, the iron ore powder A is respectively entered into a dry grinding system and a wet grinding system for processing, and the processing capacity of the dry grinding and the wet grinding is 50% each (50% of the mass of the iron ore powder ), respectively accounting for 25% of the total iron material (the fine powder mentioned in this case is all iron fine powder). In the dry grinding system, the iron ore powder A pre-mixing bin is mixed with 3% dolomite and 1% anthracite for mixed grinding. The proportion of 0-8mm before grinding accounts for 91%, and the finished product of -200 mesh accounts for 90% after grinding. , the moisture before grinding is 8.5%, and the moisture after grinding is 2.5%. In the wet grinding system, the iron ore powder A is separately compounded for grinding. The proportion from 0-8...
PUM
| Property | Measurement | Unit |
|---|---|---|
| particle diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com