Anti-adhesion low-smoke halogen-free and flame-retardant polyolefin cable material
A polyolefin cable material, anti-adhesion technology, applied in the direction of circuits, electrical components, plastic/resin/wax insulators, etc., can solve problems such as not easy to separate, casualties, toxic smoke, etc.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0053] An anti-adhesion, low-smoke, halogen-free and flame-retardant polyolefin cable material is prepared by the following method: 85g of ethylene-vinyl acetate copolymer, 65g of high-density polyethylene, 30g of magnesium hydroxide, 70g of aluminum hydroxide, 0.15g of melamine acid salt, 22g red phosphorus, 8.8g acrylic acid, 11g allyl alcohol, 23g silica with a diameter of 30nm, 7g zinc hydroxystannate with a diameter of 50nm, 21g nano-BaSO with a diameter of 30nm 4 , 1g of polylactic acid, and 1.5g of sodium hyaluronate are mixed uniformly, and mixed at a temperature of 130 ° C for 10 minutes, and then extruded and granulated at a temperature of 115 ° C using a twin-screw extruder to obtain anti-adhesion and low smoke. Halogen-free flame retardant polyolefin cable compound.
Embodiment 2
[0055] An anti-adhesion, low-smoke, halogen-free and flame-retardant polyolefin cable material is prepared in the following manner: 95 g of ethylene-vinyl acetate copolymer, 55 g of high-density polyethylene, 38 g of magnesium hydroxide, 50 g of aluminum hydroxide, 0.35 g of melamine urea acid salt, 10g red phosphorus, 17.6g acrylic acid, 22g allyl alcohol, 17g silica with 30nm diameter, 13g zinc hydroxystannate with 50nm diameter, 15g nano BaSO with 38nm diameter 4 , 2g of polylactic acid, and 0.5g of sodium hyaluronate are mixed evenly, and mixed at a temperature of 130 ° C for 10 minutes, and then extruded and pelletized at a temperature of 115 ° C using a twin-screw extruder to obtain anti-adhesion and low smoke. Halogen-free flame retardant polyolefin cable compound.
Embodiment 3
[0057] An anti-adhesion, low-smoke, halogen-free and flame-retardant polyolefin cable material is prepared in the following manner: 90 g of ethylene-vinyl acetate copolymer, 60 g of high-density polyethylene, 34 g of magnesium hydroxide, 60 g of aluminum hydroxide, 0.25 g of melamine urine acid salt, 16g red phosphorus, 13.5g acrylic acid, 16.5g allyl alcohol, 20g silica with 32.5nm diameter, 10g zinc hydroxystannate with 50nm diameter, 18g nano BaSO with 36nm diameter 4 , 1.5g of polylactic acid, and 1g of sodium hyaluronate were mixed evenly, and mixed at a temperature of 135 ° C for 12.5 minutes, and then at a temperature of 127.5 ° C, extruded and pelletized using a twin-screw extruder to obtain low anti-adhesion Smoke free halogen flame retardant polyolefin cable compound.
PUM
Property | Measurement | Unit |
---|---|---|
diameter | aaaaa | aaaaa |
diameter | aaaaa | aaaaa |
diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com