A repair method for outdoor thin-walled cast iron cultural relics
A restoration method and technology for cultural relics, applied in the field of restoration of iron cultural relics, can solve the problems of hot cracking and cold cracking at welding, accelerated corrosion reaction speed, etc., and achieve the effects of good weather resistance, high strength and good corrosion resistance.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment
[0023] A repair method for outdoor thin-walled cast iron cultural relics, including the preparation of new white cast iron repair materials, welding seal repair and rust resistance and weather resistance repair, the specific repair process is as follows:
[0024] (1) Preparation of new white cast iron repair materials
[0025] Use discarded white malleable cast iron as the base material, which contains carbon, silicon, manganese, sulfur and phosphorus elements, take 0.04kg of copper, 0.06kg of vanadium, 0.04kg of nickel, 0.06kg of aluminum, 0.02kg of cobalt, 0.02kg of zinc and 9.76kg of waste base material are mixed and batched, put into a graphite tank, melted at a high temperature of 1600°C, pour the melted molten iron into the molding sand model, remove the molding sand after cooling, and calcine and aging anneal at 300°C in a simmering furnace. A new type of white cast iron repair material is obtained.
[0026] (2) Welding, sealing and repairing
[0027] Welding in the r...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com