Preparation method and application of fullerene textile fabric
A technology for textile fabrics and fullerenes, applied in textiles, papermaking, fiber processing, etc., can solve problems such as unfavorable environmental protection, unfavorable direct skin contact, etc., and achieve the effects of removing stains, improving skin elasticity, and simple process
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0021] A preparation method for fullerene textile fabrics, comprising the following steps:
[0022] (1) Pretreatment: take the fabric that has been dyed or printed, dry it, and roll it up for later use;
[0023] (2) Fullerene finishing: put the fabric treated in step (1) into a fullerene finishing agent, and perform one-dipping and one-rolling treatment, wherein the fullerene finishing agent includes 0.01% of fullerene and 3% of hyaluronic acid , carnosine 3%, pearl powder 3%, the balance is water, the treatment process of one soaking and one rolling is bath ratio 1:20, the dipping temperature is 35°C, and the rolling rate is 75%;
[0024] (3) Styling: Put the fabric treated in step (2) into a drying and setting machine for drying and setting treatment. The temperature in the drying and setting machine is 100°C, and the normal overfeed setting is adopted, and the speed of the machine is 15m / min.
[0025] (4) Packing: the fabric processed in step (3) is rolled up and packed in...
Embodiment 2
[0027] (1) Pretreatment: take the fabric that has been dyed or printed, dry it, and roll it up for later use;
[0028] (2) Fullerene finishing: Put the fabric treated in step (1) into a fullerene finishing agent, and perform one-dipping and one-rolling treatment, wherein the fullerene finishing agent includes 1% fullerene and 5% hyaluronic acid , carnosine 4%, pearl powder 5%, the balance is water, the treatment process of one soaking and rolling is bath ratio 1:20, dipping temperature is 55°C, and rolling rate is 100%;
[0029] (3) Styling: put the fabric treated in step (2) into a drying and setting machine for drying and setting treatment. The temperature in the drying and setting machine is 105° C., adopt normal overfeed setting, and the speed of the machine is 25m / min.
[0030] (4) Packing: the fabric processed in step (3) is rolled up and packed into a warehouse.
Embodiment 3
[0032] (1) Pretreatment: take the fabric that has been dyed or printed, dry it, and roll it up for later use;
[0033] (2) Fullerene finishing: put the fabric treated in step (1) into a fullerene finishing agent, and perform one-dipping and one-rolling treatment, wherein the fullerene finishing agent includes 4% fullerene and 4% hyaluronic acid , carnosine 3.5%, pearl powder 4%, the balance is water, the treatment process of one soaking and one rolling is bath ratio 1:20, the dipping temperature is 45°C, and the rolling rate is 88%;
[0034] (3) Styling: put the fabric treated in step (2) into a drying and setting machine for drying and setting treatment. The temperature in the drying and setting machine is 103°C. Normal overfeed setting is adopted, and the speed of the machine is 20m / min.
[0035] (4) Packing: the fabric processed in step (3) is rolled up and packed into a warehouse.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology