System and method for preventing low-temperature corrosion of coal-fired boiler pipeline
A low-temperature corrosion, coal-fired boiler technology, applied in separation methods, chemical instruments and methods, dispersed particle separation, etc., can solve problems such as no feasible prevention of low-temperature corrosion of boiler pipes, and achieve a high degree of automation, accurate detection, and prevention. The effect of low temperature corrosion
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment Construction
[0024] The present invention will be further described in detail below in conjunction with specific embodiments, which are explanations of the present invention rather than limitations.
[0025] A system for preventing low-temperature corrosion of coal-fired boiler pipes according to the present invention, comprising an alkali agent spraying system 7 and SO 3 Removal of SO by spraying alkaline agent composed of 6 on-line monitoring equipment 3 system;
[0026] The alkali agent spraying system 7 is arranged at the entrance of the SCR system 2;
[0027] Wherein, the alkali agent spraying system 7 is composed of an alkali agent spray gun 8, an alkali agent storage tank 10, a pump 9, and a PLC automatic adjustment control system 11;
[0028] The alkali agent that sprays in the alkali agent spraying system 7 refers to sodium carbonate, sodium bicarbonate, calcium oxide etc. 3 Solution or powder of alkaline substances with removal effect;
[0029] The PLC automatic adjustment co...
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More 