A graphene-based material, Pythium oligandrum technology, applied in the field of biological control, can solve the problems of polluted soil and water sources, healthy diet and green environment, insignificant effects, hidden dangers of ecological safety, pesticide residues, etc., and meets the requirements of low production equipment, Good promotion and application prospects, low cost effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0023] Embodiment 1 Effect of different concentrations of graphene materials on the growth of Pythium oligandrum
[0024] The PDA liquid medium was divided into 100mL Erlenmeyer flasks, 40mL per bottle. Experimental group: Three carbon materials, graphene, graphene oxide and three-dimensional network activated carbon, were added to the liquid medium at a ratio of 5 mg / L, 50 mg / L and 100 mg / L respectively, and shaken well; the control group did not add additional, PDA liquid medium only. Three parallels were set up for each experimental group.
[0025] Put the same amount of Pythium oligandrum agent into the above-mentioned Erlenmeyer flask, and culture it in a constant temperature shaker at 28°C at 150r / min. After 5-7 days, a large amount of flocculent mycelium grew in each bottle. And when the culture medium of the experimental group became clear and translucent, the culture was stopped at the same time.
[0026] The mycelium in each Erlenmeyer flask was taken out, rinsed ...
Embodiment 2
[0027] Example 2 Preparation of Pythium oligandrum Graphene Composite Biocontrol Preparation
[0028] 1. Divide the PDA liquid medium into 100mL Erlenmeyer flasks, 40ml per bottle. Add graphene to the Erlenmeyer flask by 5mg / L, 50 mg / L and 100mg / L, and stir evenly;
[0029] 2. Add Pythium oligandrum to the liquid medium prepared in step 1, and cultivate at 28°C and 150r / min until 5-7 days later, a large number of flocculent mycelia of Pythium oligandrum in dark gray clusters grow, and when the medium is clear and translucent Stop culturing, such as figure 1 shown;
[0030] 3. Take out the mycelium, wash off the culture medium on the mycelia with deionized water, and the resulting Pythium oligandrum graphene composite biocontrol preparation.
Embodiment 3
[0031] Example 3 Preparation of Pythium oligandrum Graphene Oxide Composite Biocontrol Preparation
[0032] 1. Divide the PDA liquid medium into 100mL Erlenmeyer flasks, 40ml per bottle. Add graphene oxide to the Erlenmeyer flask at 5 mg / L, 50 mg / L and 100 mg / L, and stir evenly;
[0033] 2. Add Pythium oligandrum to the liquid medium prepared in step 1, and cultivate at 28°C and 150r / min until 5-7 days later, a large number of flocculent mycelia of Pythium oligandrum in dark gray clusters grow, and when the medium is clear and translucent stop cultivating;
[0034] 3. Take out the mycelium, wash off the culture medium on the mycelia with deionized water, and the resulting Pythium oligandrum graphene oxide composite biocontrol preparation.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com