A kind of magnetic dressing and its preparation method and application
A magnetic and magnetic layer technology, applied in bandages, absorbent pads, medical science, etc., can solve the problem of low drug efficacy, achieve low cost, improve therapeutic effect, and achieve controllable release on demand
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0046]The present invention also provides a preparation method of the magnetic dressing described in the above technical solution, comprising the following steps:
[0047] Prepare the drug-loaded layer;
[0048] Spraying magnetic layer slurry on the surface of the drug-loaded layer to form a magnetic layer, the magnetic layer slurry contains polyvinyl alcohol, gluten and iron particles to obtain a double-layer dressing;
[0049] A protective layer is formed on the surface of the double-layer dressing to obtain the magnetic dressing.
[0050] The invention prepares the drug-loaded layer.
[0051] In the present invention, the drug-loaded layer is preferably prepared by a method comprising the following steps: mixing chitosan, anti-inflammatory drug and water to obtain a hydrogel, and the mass ratio of chitosan and anti-inflammatory drug is preferably 1 :1. The specific limitations of the anti-inflammatory drug in the present invention are preferably consistent with the above...
Embodiment 1
[0072] Chitosan and bismuth potassium citrate were used to prepare the hydrogel as its drug-loading layer at a mass ratio of 1:1.
[0073] The mass ratio of gluten: iron particles: polyvinyl alcohol solution (mass fraction 10%) = 1:8:11, the particle size of iron particles is 6 μm, mix gluten, iron particles and polyvinyl alcohol solution to obtain a magnetic layer Slurry, the magnetic layer slurry is sprayed on the surface of the drug-loaded layer with a thickness of 100 μm, and then cured to form a cured dressing. The cured dressing is bent and placed on the cylindrical surface, the magnetic layer is on the inside, and the drug-loaded layer is on the outside, and it is magnetized (magnetic induction intensity is 10mT), obtain double-layer dressing, put double-layer dressing in sodium alginate solution (mass fraction 6%), then it is transferred in calcium chloride solution (mass fraction 4%), sodium alginate The mass ratio of the solution to the calcium chloride solution is 1...
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
magnetic flux density | aaaaa | aaaaa |
thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com