Environment-friendly treatment method for reducing shrinkage rate of elastic fabric and elastic fabric
An elastic fabric and environmental protection treatment technology, applied in the field of textile fabrics, can solve the problems that elastic fabrics cannot meet the shrinkage rate requirements and environmental protection requirements, reduce the shrinkage rate of elastic fabrics, etc., achieve the effects of human health and friendliness, solve the shrinkage rate, and simple process
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0058] The elastic fabric includes warp and weft, the weft is 10S (cotton 80 wool 20) wrapped with 75D spandex, and the warp is 10S cotton.
[0059] The elastic fabric is treated as follows:
[0060] Dissolve 30kg of chitosan in 1.0kg of acetic acid, add 2kg of hydrogen peroxide, ultrasonically treat with a power of 800Hz and a treatment time of 10min to obtain a first coating finishing solution.
[0061] Dissolve 10kg of peach gum, 23kg of wheat starch and 25kg of corn starch in 38kg of hot water (50°C) to obtain a mixed solution, add 2kg of citric acid and 2kg of sodium dihydrogen orthophosphate to the mixed solution to obtain a second coating finishing solution.
[0062] Apply the first coating finishing liquid on the reverse side of the elastic fabric, control the vehicle speed to 25m / min, control the liquid carrying rate to 10%, and bake at 160°C.
[0063] Continue to apply the second coating finishing liquid on the reverse side of the elastic fabric, control the vehicle...
Embodiment 2
[0065] The difference between Example 2 and Example 1 is that the elasticity of the fabric is different.
[0066] The elastic fabric includes warp yarn and weft yarn, the weft yarn is 10S (cotton 80 wool 20) wrapped with 40D spandex, and the warp yarn is 10S cotton yarn.
[0067] The elastic fabric is treated as follows:
[0068] Dissolving 45 parts of chitosan in 1.5 parts of acetic acid, adding 3 parts of hydrogen peroxide, ultrasonic treatment, power of 800Hz, treatment time of 10min, to obtain the first coating finishing solution.
[0069] 20kg of peach gum, 20kg of wheat starch and 20kg of corn starch were dissolved in 32kg of hot water (50°C) to obtain a mixed solution, and 4kg of citric acid and 4kg of sodium dihydrogen orthophosphate were added to the mixed solution to obtain a second coating finishing solution.
[0070] Apply the first coating finishing liquid on the reverse side of the elastic fabric, control the vehicle speed to 25m / min, control the liquid carrying...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com